Trabajo presentado en el European Congress and Exhibition on Advanced Materials and Processes (EUROMAT 2013), celebrado en Sevilla (España), del 8 al 13 de septiembre de 2013: High strength steels in concrete structures used as reinforcement are usually passivated due to the physical barrier that concrete provides and by a protective passive film developed on the surface by the high alkaline media. Chloride ions can break the passive film. These ions can be found dissolved in the water or in structures in marine environment. This work is focused on the study, by Electrochemical Atomic Force Microscopy (EC-AFM), of the early stages of corrosion of such steels during exposure to a sodium chloride solution in order to better understand the evo...
Atomic force microscopes (AFMs) are capable of high-resolution mapping of structures and the measure...
Corrosion is a process that involves the action of different agents on material surfaces. Corrosive ...
Corrosion of reinforcing steel has a great influence in reducing the lifetime of concrete structures...
High strength steels in concrete structures used as reinforcement are usually passivated due to the ...
Trabajo presentado en el VI International PhD Student Workshop: Durability of Reinforced Concrete fr...
Corrosion of steel constitutes a major preoccupation in the field of civil engineering and the build...
The anaerobic corrosion of mild steel in seawater was studied by atomic force microscopy (AFM). In t...
Steel in concrete is normally protected against corrosion due to a thin and dense passive layer form...
This paper presents a study of AISI 1040 steel corrosion in aqueous electrolyte of acetic acid buffe...
International audienceThis paper deals with the characterisation by means of electrochemical, gravim...
Pitting corrosion has been studied for more than 5 decades by many different techniques, which have ...
Atomic force microscopy (PFM), invented in 1986, has found widespread use in science. The technique...
AbstractIn the study characterization of steel corrosion in concrete at the macro- and micro-level w...
Seawater and sea sand concrete (SWSSC) is an environmentally friendly alternative to ordinary Portla...
Dual-phase high carbon steel is widely used in mining and in chemical industry applications in highl...
Atomic force microscopes (AFMs) are capable of high-resolution mapping of structures and the measure...
Corrosion is a process that involves the action of different agents on material surfaces. Corrosive ...
Corrosion of reinforcing steel has a great influence in reducing the lifetime of concrete structures...
High strength steels in concrete structures used as reinforcement are usually passivated due to the ...
Trabajo presentado en el VI International PhD Student Workshop: Durability of Reinforced Concrete fr...
Corrosion of steel constitutes a major preoccupation in the field of civil engineering and the build...
The anaerobic corrosion of mild steel in seawater was studied by atomic force microscopy (AFM). In t...
Steel in concrete is normally protected against corrosion due to a thin and dense passive layer form...
This paper presents a study of AISI 1040 steel corrosion in aqueous electrolyte of acetic acid buffe...
International audienceThis paper deals with the characterisation by means of electrochemical, gravim...
Pitting corrosion has been studied for more than 5 decades by many different techniques, which have ...
Atomic force microscopy (PFM), invented in 1986, has found widespread use in science. The technique...
AbstractIn the study characterization of steel corrosion in concrete at the macro- and micro-level w...
Seawater and sea sand concrete (SWSSC) is an environmentally friendly alternative to ordinary Portla...
Dual-phase high carbon steel is widely used in mining and in chemical industry applications in highl...
Atomic force microscopes (AFMs) are capable of high-resolution mapping of structures and the measure...
Corrosion is a process that involves the action of different agents on material surfaces. Corrosive ...
Corrosion of reinforcing steel has a great influence in reducing the lifetime of concrete structures...