Ab initio total energy calculations based on the exact muffin-tin orbitals method, combined with the coherent potential approximation, have been used to study the thermodynamical and elastic properties of substitutional refractory Ru1-xNixAl alloys. We have found that the elastic constants C- and C-11 exhibit pronounced peculiarities near the concentration of about 40 at. % Ni, which we ascribe to electronic topological transitions. Our suggestion is supported by the Fermi surface calculations in the whole concentration range. Results of our calculations show that one can design Ru-Ni-Al alloys substituting Ru by Ni (up to 40 at. %) with almost invariable elastic constants and reduced density.Original Publication:I D Bleskov, E A Smirnova, ...
It is well established that Re and Ru additions to Ni-base superalloys result in improved creep perf...
It is well established that Re and Ru additions to Ni-base superalloys result in improved creep perf...
It is well established that Re and Ru additions to Ni-base superalloys result in improved creep perf...
Ab initio total energy calculations based on the exact muffin-tin orbitals method, combined with the...
Contains fulltext : 76051.pdf (publisher's version ) (Open Access)3 p
The effect of substitutional alloying of Re on elastic properties of B2 NiAl has been studied using ...
Using the exact muffin-tin orbitals method in conjunction with the coherent potential approximation,...
In this paper, the basic electronic structures and elastic properties of Ni3Al doping with alloying ...
In this paper, the basic electronic structures and elastic properties of Ni3Al doping with alloying ...
Any property of a material is a function of its microstructure and microstructure is a function of m...
Any property of a material is a function of its microstructure and microstructure is a function of m...
The electronic structure, interatomic bonding, and mechanical properties of two supercell models of ...
The structural, electronic, elastic, mechanical and thermal properties of transition metal aluminide...
Advanced mechanical properties of Ni-based superalloys strongly depend on the site preferences of al...
Nickel based superalloys have superior high temperature mechanical strength, corrosion and creep res...
It is well established that Re and Ru additions to Ni-base superalloys result in improved creep perf...
It is well established that Re and Ru additions to Ni-base superalloys result in improved creep perf...
It is well established that Re and Ru additions to Ni-base superalloys result in improved creep perf...
Ab initio total energy calculations based on the exact muffin-tin orbitals method, combined with the...
Contains fulltext : 76051.pdf (publisher's version ) (Open Access)3 p
The effect of substitutional alloying of Re on elastic properties of B2 NiAl has been studied using ...
Using the exact muffin-tin orbitals method in conjunction with the coherent potential approximation,...
In this paper, the basic electronic structures and elastic properties of Ni3Al doping with alloying ...
In this paper, the basic electronic structures and elastic properties of Ni3Al doping with alloying ...
Any property of a material is a function of its microstructure and microstructure is a function of m...
Any property of a material is a function of its microstructure and microstructure is a function of m...
The electronic structure, interatomic bonding, and mechanical properties of two supercell models of ...
The structural, electronic, elastic, mechanical and thermal properties of transition metal aluminide...
Advanced mechanical properties of Ni-based superalloys strongly depend on the site preferences of al...
Nickel based superalloys have superior high temperature mechanical strength, corrosion and creep res...
It is well established that Re and Ru additions to Ni-base superalloys result in improved creep perf...
It is well established that Re and Ru additions to Ni-base superalloys result in improved creep perf...
It is well established that Re and Ru additions to Ni-base superalloys result in improved creep perf...