Communication to : ICAF'99, Seattle (USA), July 12-16, 1999SIGLEAvailable from INIST (FR), Document Supply Service, under shelf-number : 22419, issue : a.1999 n.95 / INIST-CNRS - Institut de l'Information Scientifique et TechniqueFRFranc
The introduction of single crystal casting techniques has led to the development of existing nickel-...
Tire de : 3rd int. conf. on 'Constitutive laws for engineering materials, theory and applications', ...
The mechanical behavior of a new single-crystal nickel-based superalloy for industrial gas turbine (...
Presented at the International Symposium on Superalloys, USA, September 2000Available from British L...
Cast single-crystal superalloys are being used as turbine blades in modern aeroengines with [001] ax...
A physics based model has been developed that accounts for the principal features of anisotropic cre...
Paru dans 17th ICAS Congress, Stockolm (Sweden), September 9-14, 1990SIGLEAvailable at INIST (FR), D...
Abstract: A physics based model has been developed that accounts for the principal features of aniso...
Communication to : international symposium on materials ageing and life management (ISOMALM 2000), K...
Presented at Superalloys 2000, Seven Springs, USA, September 2000Available from British Library Docu...
La tenue au fluage des aubes de turbine haute pression est une problématique de premier ordre vis-à-...
Published in : Advances in Multiaxial Fatigue, Mc Dowells/Ellis, editors, ASTM, September 1993, pp. ...
In this study, the TMF stress relaxation and creep behavior at 1023 K and 1223 K (750 °C and 950 °C)...
Communication to : 11th European conference on fractures, Poitiers (France), september 3-6, 1996SIGL...
Directionally solidified (DS) Ni-base superalloys are commonly used as gas turbine materials to prim...
The introduction of single crystal casting techniques has led to the development of existing nickel-...
Tire de : 3rd int. conf. on 'Constitutive laws for engineering materials, theory and applications', ...
The mechanical behavior of a new single-crystal nickel-based superalloy for industrial gas turbine (...
Presented at the International Symposium on Superalloys, USA, September 2000Available from British L...
Cast single-crystal superalloys are being used as turbine blades in modern aeroengines with [001] ax...
A physics based model has been developed that accounts for the principal features of anisotropic cre...
Paru dans 17th ICAS Congress, Stockolm (Sweden), September 9-14, 1990SIGLEAvailable at INIST (FR), D...
Abstract: A physics based model has been developed that accounts for the principal features of aniso...
Communication to : international symposium on materials ageing and life management (ISOMALM 2000), K...
Presented at Superalloys 2000, Seven Springs, USA, September 2000Available from British Library Docu...
La tenue au fluage des aubes de turbine haute pression est une problématique de premier ordre vis-à-...
Published in : Advances in Multiaxial Fatigue, Mc Dowells/Ellis, editors, ASTM, September 1993, pp. ...
In this study, the TMF stress relaxation and creep behavior at 1023 K and 1223 K (750 °C and 950 °C)...
Communication to : 11th European conference on fractures, Poitiers (France), september 3-6, 1996SIGL...
Directionally solidified (DS) Ni-base superalloys are commonly used as gas turbine materials to prim...
The introduction of single crystal casting techniques has led to the development of existing nickel-...
Tire de : 3rd int. conf. on 'Constitutive laws for engineering materials, theory and applications', ...
The mechanical behavior of a new single-crystal nickel-based superalloy for industrial gas turbine (...