Tire de : 3rd int. conf. on 'Constitutive laws for engineering materials, theory and applications', Tuscon (Arizone, USA), january 7-12, 1991Available at INIST (FR), Document Supply Service, under shelf-number : 22419, issue : a.1991 n.6 / INIST-CNRS - Institut de l'Information Scientifique et TechniqueSIGLEFRFranc
Current gas turbine engines utilize large single crystal superalloy components in the hot section. S...
Single crystal materials are being used in gas turbine airfoils and are candidates for other hot sec...
Nickel-base superalloy blades of the first rotor stage in a gas turbine have to withstand extremely ...
Paru dans 17th ICAS Congress, Stockolm (Sweden), September 9-14, 1990SIGLEAvailable at INIST (FR), D...
Communication to : ICAF'99, Seattle (USA), July 12-16, 1999SIGLEAvailable from INIST (FR), Document ...
A unified viscoplastic constitutive relation based on crystallographic slip theory was developed for...
Graphite material is used extensively in nuclear reactors however the material has a limited strain ...
This volume consists of a collection of chapters by recognized experts to provide a comprehensive fu...
The purpose of this research is to develop a new tool for mechanical design and analysis of single c...
In this work, a constitutive theory is developed, within the context of continuum mechanics, to desc...
Presented at the International Symposium on Superalloys, USA, September 2000Available from British L...
The additively manufactured materials show anisotropic mechanical properties. In the present paper, ...
A constitutive theory is presented for representing the anisotropic viscoplastic behavior of high te...
Single crystal superalloys are actively being considered for use in industrial gas turbines and it i...
A physics based model has been developed that accounts for the principal features of anisotropic cre...
Current gas turbine engines utilize large single crystal superalloy components in the hot section. S...
Single crystal materials are being used in gas turbine airfoils and are candidates for other hot sec...
Nickel-base superalloy blades of the first rotor stage in a gas turbine have to withstand extremely ...
Paru dans 17th ICAS Congress, Stockolm (Sweden), September 9-14, 1990SIGLEAvailable at INIST (FR), D...
Communication to : ICAF'99, Seattle (USA), July 12-16, 1999SIGLEAvailable from INIST (FR), Document ...
A unified viscoplastic constitutive relation based on crystallographic slip theory was developed for...
Graphite material is used extensively in nuclear reactors however the material has a limited strain ...
This volume consists of a collection of chapters by recognized experts to provide a comprehensive fu...
The purpose of this research is to develop a new tool for mechanical design and analysis of single c...
In this work, a constitutive theory is developed, within the context of continuum mechanics, to desc...
Presented at the International Symposium on Superalloys, USA, September 2000Available from British L...
The additively manufactured materials show anisotropic mechanical properties. In the present paper, ...
A constitutive theory is presented for representing the anisotropic viscoplastic behavior of high te...
Single crystal superalloys are actively being considered for use in industrial gas turbines and it i...
A physics based model has been developed that accounts for the principal features of anisotropic cre...
Current gas turbine engines utilize large single crystal superalloy components in the hot section. S...
Single crystal materials are being used in gas turbine airfoils and are candidates for other hot sec...
Nickel-base superalloy blades of the first rotor stage in a gas turbine have to withstand extremely ...