The lifetime of an aluminum electrolysis cell is mainly determined by the cathode wear, especially for high amperage cells utilizing graphitized carbon cathodes. The cathode wear mechanisms are, however, complex and still subject to debate. Laboratory tests using inverted cell configurations have previously been used to study commercial cathode materials. Here we report on results obtained in the last 5 years for three different commercial cathode materials. The current density applied in the tests was in the range from 0 to 2 A/cm2 and the rotation speed of the cathode was from 0 to 125 rpm, corresponding to surface velocity 0-19.6 cm/s. The wear mechanisms with respect to current density, limiting current of Al4C3 formation and mass trans...
The present study is an investigation of the effect of pulse duration on properties of coatings for...
The current distribution in a fresh aluminum electrolytic cell with slotted carbons is investigated ...
Cathode wear is considered as one of the key factors for limiting the lifetime of aluminium electrol...
The lifetime of an aluminum electrolysis cell is mainly determined by the cathode wear, especially f...
The aluminium smelters are continually trying to increase their production either by designing high ...
To investigate cathode wear, an autopsy of a shutdown aluminium electrolysis cell was conducted. The...
Autopsies of six spent potlinings with different carbon cathode block grades, amperage regimes and c...
Autopsies of six spent potlinings with different carbon cathode block grades, amperage regimes and c...
Uneven cathode wear is one of the key challenges for the lifetime of aluminium electrolysis cells. H...
Aluminum cathodes have long been used for the electrowinning of zinc from zinc sulfatesulfuric acid...
Interaction between electrolyte and carbon cathodes during the electrolytic production of aluminium ...
The extent to which the carbon cathode is wetted by molten electrolyte or molten aluminium metal is ...
The final publication is available at Springer via http://dx.doi.org/10.1007/978-3-319-72284-9_159Th...
Electrocoagulation (EC) is a sustainable water treatment process involving the generation of coagula...
It is now rather well established that the cathode panel erosion rate is proportional to the current...
The present study is an investigation of the effect of pulse duration on properties of coatings for...
The current distribution in a fresh aluminum electrolytic cell with slotted carbons is investigated ...
Cathode wear is considered as one of the key factors for limiting the lifetime of aluminium electrol...
The lifetime of an aluminum electrolysis cell is mainly determined by the cathode wear, especially f...
The aluminium smelters are continually trying to increase their production either by designing high ...
To investigate cathode wear, an autopsy of a shutdown aluminium electrolysis cell was conducted. The...
Autopsies of six spent potlinings with different carbon cathode block grades, amperage regimes and c...
Autopsies of six spent potlinings with different carbon cathode block grades, amperage regimes and c...
Uneven cathode wear is one of the key challenges for the lifetime of aluminium electrolysis cells. H...
Aluminum cathodes have long been used for the electrowinning of zinc from zinc sulfatesulfuric acid...
Interaction between electrolyte and carbon cathodes during the electrolytic production of aluminium ...
The extent to which the carbon cathode is wetted by molten electrolyte or molten aluminium metal is ...
The final publication is available at Springer via http://dx.doi.org/10.1007/978-3-319-72284-9_159Th...
Electrocoagulation (EC) is a sustainable water treatment process involving the generation of coagula...
It is now rather well established that the cathode panel erosion rate is proportional to the current...
The present study is an investigation of the effect of pulse duration on properties of coatings for...
The current distribution in a fresh aluminum electrolytic cell with slotted carbons is investigated ...
Cathode wear is considered as one of the key factors for limiting the lifetime of aluminium electrol...