The present work was performed on experimental Al-Si near eutectic cast alloys, with different additives mainly Fe, Mg, Mn, Cr, Sr and P. The alloys were cooled at 0\ub78\ub0C s-1, very close to equilibrium conditions. Precipitated phases, primarily Fe, Cu, Mg and Sr based intermetallics, were examined. Although the phases reported in the present work were documented previously, the range of chemical composition of each phase was confirmed using an electron probe microanalyser equipped with wavelength dispersive spectroscopy and electron dispersive X-ray spectroscopy facilities.Peer reviewed: YesNRC publication: Ye
The solidification of Al-4.6Cu-0.5Fe-0.5Mn (206 type) cast alloy has been studied using Thermal Anal...
Available from British Library Document Supply Centre-DSC:DX217142 / BLDSC - British Library Documen...
The solidification structures of Al-Cu 206 cast alloys at a high iron level of 0.5 pct were systemat...
Post-eutectic reactions occurring in Al-Si hypoeutectic alloys containing different proportions of C...
Al-Si based casting alloys are widely used for piston applications. This is due to their combination...
In the present study, four Al-Mg-Mn 5xxx alloys with different Mg levels (2-5 wt.%) were investigate...
Iron is the most common and detrimental impurity in aluminum casting alloys and has long been associ...
The intermetallic phases present in high-purity and commercial purity Al-Mn alloys(up to 2 Mn) ...
Applications of Al-Si cast alloys in recent years have increased especially in the automotive indust...
The influence of Cu content (0, 0.5 and 1 wt%) on the nature of intermetallic phases was carefully i...
Recent studies have shown that the beta-Al5FeSi and theta-Al2Cu phase intermetallic particles are re...
Aluminium alloys that contain Si, Mg, Fe, Mn and/or Cu usually contain one or more types of intermet...
Iron and silicon are the major impurities in the 1000 series of wrought aluminum alloys. As the alum...
Abstract: This study focuses on primary impurities, called intermetallics, in the microstructure of ...
Structure and chemical composition of intermetallic phases in unmodified and Sr modified Al 10Si 0.3...
The solidification of Al-4.6Cu-0.5Fe-0.5Mn (206 type) cast alloy has been studied using Thermal Anal...
Available from British Library Document Supply Centre-DSC:DX217142 / BLDSC - British Library Documen...
The solidification structures of Al-Cu 206 cast alloys at a high iron level of 0.5 pct were systemat...
Post-eutectic reactions occurring in Al-Si hypoeutectic alloys containing different proportions of C...
Al-Si based casting alloys are widely used for piston applications. This is due to their combination...
In the present study, four Al-Mg-Mn 5xxx alloys with different Mg levels (2-5 wt.%) were investigate...
Iron is the most common and detrimental impurity in aluminum casting alloys and has long been associ...
The intermetallic phases present in high-purity and commercial purity Al-Mn alloys(up to 2 Mn) ...
Applications of Al-Si cast alloys in recent years have increased especially in the automotive indust...
The influence of Cu content (0, 0.5 and 1 wt%) on the nature of intermetallic phases was carefully i...
Recent studies have shown that the beta-Al5FeSi and theta-Al2Cu phase intermetallic particles are re...
Aluminium alloys that contain Si, Mg, Fe, Mn and/or Cu usually contain one or more types of intermet...
Iron and silicon are the major impurities in the 1000 series of wrought aluminum alloys. As the alum...
Abstract: This study focuses on primary impurities, called intermetallics, in the microstructure of ...
Structure and chemical composition of intermetallic phases in unmodified and Sr modified Al 10Si 0.3...
The solidification of Al-4.6Cu-0.5Fe-0.5Mn (206 type) cast alloy has been studied using Thermal Anal...
Available from British Library Document Supply Centre-DSC:DX217142 / BLDSC - British Library Documen...
The solidification structures of Al-Cu 206 cast alloys at a high iron level of 0.5 pct were systemat...