The determination of mechanical properties of materials at elevated temperature presents difficulties, particularly when the material to be tested is subject to oxidation. Various methods have been employed to permit the evaluation of high temperature creep properties. The method described in this paper was developed on the basis of modifications of a technique developed for the protection of high temperature fatigue specimens. The method involves encasing the creep specimen in a flexible capsule which is capable of withstanding exposure to the atmosphere for extended periods at temperatures up to 1000C. Extensive testing of materials such as uranium and tantalum has provided the basis for claims relative to the effectiveness of this techni...
Creep strength and fracture resistance are two properties that are critical in the selection and opt...
Structural metals used in plant components are subject to aging from a combination of fatigue, creep...
The problems of obtaining accurate strain data, providing reliable temperature control, and affordin...
"Chemistry-General (UC-4) TID 4500, August 1, 1959.""October 1959.""Ames Laboratory at Iowa State Un...
The special test equipment and procedures developed for the evaluation of ultrashort-Hme elevated-te...
The aim of this paper is to explain the process realized during the design and construction of a cre...
THE demand for heat and creep resisting steels and other special alloys has immensely increased i...
This is an investigation on tensile testing dealing with the serious weakening effect which occurs a...
In view of the rapidly increasing demands for creep resistant steels and alloys in the country a com...
Many components in conventional and nuclear power plant, aero-engines, chemical plant etc., operate ...
Many components in conventional and nuclear power plant, aero-engines, chemical plant etc., operate ...
Many components in conventional and nuclear power plant, aero-engines, chemical plant etc., operate ...
This research proposes a methodology for accelerated testing in the area of high-temperature creep a...
A review is made of the principal concepts of high temperature fatigue behavior of metals as obtaine...
The origins of thermal fatigue are first considered, with reference to the turbine blades of jet tur...
Creep strength and fracture resistance are two properties that are critical in the selection and opt...
Structural metals used in plant components are subject to aging from a combination of fatigue, creep...
The problems of obtaining accurate strain data, providing reliable temperature control, and affordin...
"Chemistry-General (UC-4) TID 4500, August 1, 1959.""October 1959.""Ames Laboratory at Iowa State Un...
The special test equipment and procedures developed for the evaluation of ultrashort-Hme elevated-te...
The aim of this paper is to explain the process realized during the design and construction of a cre...
THE demand for heat and creep resisting steels and other special alloys has immensely increased i...
This is an investigation on tensile testing dealing with the serious weakening effect which occurs a...
In view of the rapidly increasing demands for creep resistant steels and alloys in the country a com...
Many components in conventional and nuclear power plant, aero-engines, chemical plant etc., operate ...
Many components in conventional and nuclear power plant, aero-engines, chemical plant etc., operate ...
Many components in conventional and nuclear power plant, aero-engines, chemical plant etc., operate ...
This research proposes a methodology for accelerated testing in the area of high-temperature creep a...
A review is made of the principal concepts of high temperature fatigue behavior of metals as obtaine...
The origins of thermal fatigue are first considered, with reference to the turbine blades of jet tur...
Creep strength and fracture resistance are two properties that are critical in the selection and opt...
Structural metals used in plant components are subject to aging from a combination of fatigue, creep...
The problems of obtaining accurate strain data, providing reliable temperature control, and affordin...