The thermal degradation of three monosubstituted hexacarbonyl complexes, M(CO)5py (where M=Cr, Mo, and W; py=pyridine) has been studied by thermogravimetry (TG) and differential scanning calorimetry (DSC) and their results reported. It was found that for each of the three complexes studied, the starting material M(CO)6 was formed which immediately sublimed unchanged with or without concomitant loss of carbonyl (CO) ligands to give the first large weight loss step. This was closely followed by the volatilisation of the pyridine ligands and at higher temperatures the loss of further CO ligands. The enthalpy changes associated with the above-mentioned steps are reported. The conversion of M(CO)5py to M(CO)6 and other products was confirmed by ...
Photoprocesses, both photochemical and photophysical, have been studied for a variety of substituted...
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)Interaction of some bivalent met...
The behaviour of the photochemically produced tungsten pentacarbonyl is investigated by laser flash ...
Thermogravimetric and differential scanning calorimetric studies on M(CO)5(PPh3) (M = Cr,Mo,W) revea...
The thermal degradation of three monosubstituted hexacarbonyl complexes, M(CO)5(dppm) (where M=Cr, M...
The effect of (CH3)3NO·2H2O on the thermal degradation of Mo(CO)6 in nitrogen was studied by thermog...
Enthalpies of ligand substitution based on reaction of (cycloheptatriene)Cr(CO)3, (naphthalene)Cr(CO...
Thermal decomposition of the singly-bridged complexes Mo2(CO)10[μ-Ph2P(CH2)nPPh2] (n=4, 5, 6) has be...
The heats of decomposition of some transition metal complexes have been measured by (a) adiabatic re...
Thermal decarbonylation of the unidentate complexes M(CO)5(η1-dppf) (M = Cr, Mo, W) and Fe(CO)4(η1-d...
Chemical studies of superheavy elements require fast and efficient techniques, due to short half-liv...
The thermal decompositions of 15 solid products of reactions of chromyl chloride and chromyl acetate...
Singly-bridging diphosphine complexes M2(CO)10(μ-dppp) (M Cr, W; dppp Ph2P(CH2)3PPh2) have been isol...
Thermal behavior of Cu(II), U(VI), Mn(II) and Ni(II) complexes with 2',2"'-(2,6-pyridinediyldiethyli...
Thermal behavior of Co(II), Cd(II), and Zn(II) complexes with N-benzyloxycarbonylglycinato ligand wa...
Photoprocesses, both photochemical and photophysical, have been studied for a variety of substituted...
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)Interaction of some bivalent met...
The behaviour of the photochemically produced tungsten pentacarbonyl is investigated by laser flash ...
Thermogravimetric and differential scanning calorimetric studies on M(CO)5(PPh3) (M = Cr,Mo,W) revea...
The thermal degradation of three monosubstituted hexacarbonyl complexes, M(CO)5(dppm) (where M=Cr, M...
The effect of (CH3)3NO·2H2O on the thermal degradation of Mo(CO)6 in nitrogen was studied by thermog...
Enthalpies of ligand substitution based on reaction of (cycloheptatriene)Cr(CO)3, (naphthalene)Cr(CO...
Thermal decomposition of the singly-bridged complexes Mo2(CO)10[μ-Ph2P(CH2)nPPh2] (n=4, 5, 6) has be...
The heats of decomposition of some transition metal complexes have been measured by (a) adiabatic re...
Thermal decarbonylation of the unidentate complexes M(CO)5(η1-dppf) (M = Cr, Mo, W) and Fe(CO)4(η1-d...
Chemical studies of superheavy elements require fast and efficient techniques, due to short half-liv...
The thermal decompositions of 15 solid products of reactions of chromyl chloride and chromyl acetate...
Singly-bridging diphosphine complexes M2(CO)10(μ-dppp) (M Cr, W; dppp Ph2P(CH2)3PPh2) have been isol...
Thermal behavior of Cu(II), U(VI), Mn(II) and Ni(II) complexes with 2',2"'-(2,6-pyridinediyldiethyli...
Thermal behavior of Co(II), Cd(II), and Zn(II) complexes with N-benzyloxycarbonylglycinato ligand wa...
Photoprocesses, both photochemical and photophysical, have been studied for a variety of substituted...
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)Interaction of some bivalent met...
The behaviour of the photochemically produced tungsten pentacarbonyl is investigated by laser flash ...