Different compositions of visible-light-curable triethylene glycol dimethacrylate/bisglycidyl methacrylate copolymers used in dental resin formulations were prepared through copolymerization photoinitiated by a camphorquinone/ethyl 4-dimethylaminobenzoate system irradiated with an Ultrablue IS light-emitting diode. The obtained copolymers were evaluated with differential scanning calorimetry. From the data for the heat of polymerization, before and after light exposure, obtained from exothermic differential scanning calorimetry curves, the light polymerization efficiency or degree of conversion of double bonds was calculated. The glass-transition temperature also was determined before and after photopolymerization. After the photopolymeriza...
Aim of magister´s thesis was to study reaction kinetics of dental materials. Thesis was focused on d...
Triethylene glycol dimethacrylate (TEGDMA) was formulated with 1.0 wt % (±)-camphorquinone (CQ) as a...
We have investigated the thermal and structural properties of different commercial dental resins: Fi...
Different compositions of visible-light-curable triethylene glycol dimethacrylate/bisglycidyl methac...
The aim of this work was to evaluate the effect of the storage time on the thermal properties of tri...
The photoinitiated polymerization of a dental formulation is composed of Mixture of monomers 75%Bis-...
OBJECTIVES: This work aims to review the key factors affecting the polymerization efficiency of ligh...
The main aim of the study was to implement the most reliable method of measuring the degrees of conv...
Mechanical properties of composers would be obtained mainly by photopolymerization by visible light ...
The work is focused on monitoring the impact of several different types of polymerization lamps to h...
Introduction. Polymerization of light-cured dental materials used for restoration of hard tooth tiss...
Three novel phosphonated methacrylate monomers have been synthesized and studied for use in dental a...
The purpose of this study was to evaluate the temperature increase during the polymerization process...
To evaluate the effects of Type I and Type II photoinitiator systems on curing efficiency, degree of...
Objective: The present study was carried out in order to assess the suitability of N,N-dimethylamino...
Aim of magister´s thesis was to study reaction kinetics of dental materials. Thesis was focused on d...
Triethylene glycol dimethacrylate (TEGDMA) was formulated with 1.0 wt % (±)-camphorquinone (CQ) as a...
We have investigated the thermal and structural properties of different commercial dental resins: Fi...
Different compositions of visible-light-curable triethylene glycol dimethacrylate/bisglycidyl methac...
The aim of this work was to evaluate the effect of the storage time on the thermal properties of tri...
The photoinitiated polymerization of a dental formulation is composed of Mixture of monomers 75%Bis-...
OBJECTIVES: This work aims to review the key factors affecting the polymerization efficiency of ligh...
The main aim of the study was to implement the most reliable method of measuring the degrees of conv...
Mechanical properties of composers would be obtained mainly by photopolymerization by visible light ...
The work is focused on monitoring the impact of several different types of polymerization lamps to h...
Introduction. Polymerization of light-cured dental materials used for restoration of hard tooth tiss...
Three novel phosphonated methacrylate monomers have been synthesized and studied for use in dental a...
The purpose of this study was to evaluate the temperature increase during the polymerization process...
To evaluate the effects of Type I and Type II photoinitiator systems on curing efficiency, degree of...
Objective: The present study was carried out in order to assess the suitability of N,N-dimethylamino...
Aim of magister´s thesis was to study reaction kinetics of dental materials. Thesis was focused on d...
Triethylene glycol dimethacrylate (TEGDMA) was formulated with 1.0 wt % (±)-camphorquinone (CQ) as a...
We have investigated the thermal and structural properties of different commercial dental resins: Fi...