In this work the catalytic performance of Cu(5%)/Al2O3 catalysts prepared by wet impregnation and calcined at three different temperatures, 400 ºC (WI 400), 650 ºC (WI 650) and 900 ºC (WI 900), was analyzed. These materials were tested in the phenol wet oxidation reaction using H2O2 (0.22 or 0.88 M) as an oxidizing agent, 1000 mg/L of phenol at 70 °C and atmospheric pressure. A complete conversion of phenol and a high extent of phenol mineralization were obtained for the three catalysts. Surface Cu2+ species suffered a reduction process during the catalytic reaction due to the drop of the pH value and a fraction of the reduced copper was leached to the liquid phase. Despite this, the increment in the calcination temperature produced a decre...
Catalytic wet oxidation (CWO) of ferulic acid (a model lignin compound) was investigated at low temp...
Various processes can be used for the treatment of wastewater, but the one we feel to be important a...
The wet air oxidation of phenol aqueous solutions (5 g/L) has been studied in a trickle bed reactor ...
Three 5% CuO/CeO2 catalysts were synthesized by sol–gel, precipitation and combustion methods, follo...
An optimized wet-proofed catalyst was prepared by successive immersion steps of conventional 37% CuO...
This work aims to study the catalytic performance of Cu/Al2O3 catalysts in the catalytic reaction of...
A large variety of catalytic systems have been studied for the catalytic wet air oxidation of phenol...
Two wet-proofed catalysts were prepared by subsequent coating steps with polytetrafluoroethylene fib...
The oxidation of phenol solutions (5 g/L) has been studied in a semibatch autoclave reactor. Activit...
Two CuO/gAl2O3 catalysts were synthesized at different calcinations temperatures and used for the ox...
The performance of a commercial CuO/alumina catalyst used in the catalytic wet peroxide oxidation (C...
The present study investigated the efficiency of catalytic wet oxidation (CWO) for the destruction o...
Improved Fe2O3/Al2O3 catalysts were studied for the catalytic oxidation of concentrated phenol solut...
Structured catalysts are more suitable than powder catalysts for liquid phase reactions since their ...
Liquid phase catalytic oxidation of phenol was carried out over Cu-Ni-Al hydrotalcite at ambient tem...
Catalytic wet oxidation (CWO) of ferulic acid (a model lignin compound) was investigated at low temp...
Various processes can be used for the treatment of wastewater, but the one we feel to be important a...
The wet air oxidation of phenol aqueous solutions (5 g/L) has been studied in a trickle bed reactor ...
Three 5% CuO/CeO2 catalysts were synthesized by sol–gel, precipitation and combustion methods, follo...
An optimized wet-proofed catalyst was prepared by successive immersion steps of conventional 37% CuO...
This work aims to study the catalytic performance of Cu/Al2O3 catalysts in the catalytic reaction of...
A large variety of catalytic systems have been studied for the catalytic wet air oxidation of phenol...
Two wet-proofed catalysts were prepared by subsequent coating steps with polytetrafluoroethylene fib...
The oxidation of phenol solutions (5 g/L) has been studied in a semibatch autoclave reactor. Activit...
Two CuO/gAl2O3 catalysts were synthesized at different calcinations temperatures and used for the ox...
The performance of a commercial CuO/alumina catalyst used in the catalytic wet peroxide oxidation (C...
The present study investigated the efficiency of catalytic wet oxidation (CWO) for the destruction o...
Improved Fe2O3/Al2O3 catalysts were studied for the catalytic oxidation of concentrated phenol solut...
Structured catalysts are more suitable than powder catalysts for liquid phase reactions since their ...
Liquid phase catalytic oxidation of phenol was carried out over Cu-Ni-Al hydrotalcite at ambient tem...
Catalytic wet oxidation (CWO) of ferulic acid (a model lignin compound) was investigated at low temp...
Various processes can be used for the treatment of wastewater, but the one we feel to be important a...
The wet air oxidation of phenol aqueous solutions (5 g/L) has been studied in a trickle bed reactor ...