This paper describes some aspects ofthe processes involved in the development of high-quality probabilistic models for corrosion loss and for maximum pit depth for steels exposed to marine environments. Such models increasingly are required for advanced infrastructure life-cycle management to predict likely future levels of deterioration and for the setting of rational inspection regimes. Most models currently available are empirical. They have high levels of uncertainty. The models described herein are based on appropriate levels of representation of underlying corrosion science fundamentals, including the recognition of the important role of microbiological activity and model calibration using a probabilistic approach to data interpretati...
High strength steels such as X80 steels have recently been used more frequently in production of off...
Pitting corrosion is one of the main threats in the pressure vessels integrity and also causes the f...
This paper demonstrates the application of the probability distributions in modelling the time-depen...
With the increasing emphasis on attempting to retain in service ageing infrastructure models for the...
To derive the extreme value statistics for maximum depth of pits in pitting corrosion, it is convent...
The modelling of both short- and long-term corrosion loss and maximum pit depth is increasingly of i...
It is proposed that for immersion corrosion conditions extreme pit depths are those resulting from i...
It is proposed that for immersion corrosion conditions extreme pit depths are those resulting from i...
Research Doctorate - Doctor of Philosophy (PhD)Natural deterioration of steel structures exposed to ...
High strength steels such as X80 steels have recently been used more frequently in production of off...
For the management of infrastructure over long periods of time and for the assessment of infrastruct...
Maximum pit depth is a matter of considerable practical interest. In applied corrosion mechanics it ...
High strength steels such as X80 steels have recently been used more frequently in production of off...
High strength steels such as X80 steels have recently been used more frequently in production of off...
High strength steels such as X80 steels have recently been used more frequently in production of off...
High strength steels such as X80 steels have recently been used more frequently in production of off...
Pitting corrosion is one of the main threats in the pressure vessels integrity and also causes the f...
This paper demonstrates the application of the probability distributions in modelling the time-depen...
With the increasing emphasis on attempting to retain in service ageing infrastructure models for the...
To derive the extreme value statistics for maximum depth of pits in pitting corrosion, it is convent...
The modelling of both short- and long-term corrosion loss and maximum pit depth is increasingly of i...
It is proposed that for immersion corrosion conditions extreme pit depths are those resulting from i...
It is proposed that for immersion corrosion conditions extreme pit depths are those resulting from i...
Research Doctorate - Doctor of Philosophy (PhD)Natural deterioration of steel structures exposed to ...
High strength steels such as X80 steels have recently been used more frequently in production of off...
For the management of infrastructure over long periods of time and for the assessment of infrastruct...
Maximum pit depth is a matter of considerable practical interest. In applied corrosion mechanics it ...
High strength steels such as X80 steels have recently been used more frequently in production of off...
High strength steels such as X80 steels have recently been used more frequently in production of off...
High strength steels such as X80 steels have recently been used more frequently in production of off...
High strength steels such as X80 steels have recently been used more frequently in production of off...
Pitting corrosion is one of the main threats in the pressure vessels integrity and also causes the f...
This paper demonstrates the application of the probability distributions in modelling the time-depen...