Heat-up times derived from studies on the ignition characteristics of a few model composite solid propellants, containing polystyrene, carboxy-terminated polybutadiene, plasticised polyvinyl chloride and polyphenol formaldehyde as binders, show that they are directly proportional to the mass of the sample and inversely proportional to the heat flux. Propellant weight-loss prior to ignition and high pressure ignition temperature data on the propellants, ammonium per chlorate, and binders show that the ignition is governed by the gasification of the binder pyrolysis products. The activation energy for the gasification of the pyrolysed polymer products corresponds to their ignition behaviour suggesting that propellant ignition is con...
Ignition of a composite aluminised propellant (AP-HTPB-Al) in stagnant hot air is analysed theoreti...
The propellant composition is one of several parameter that influencing the temperature sensitivity ...
Calorimetric value and ignition temp. of carboxy-terminated polybutadiene$/NH_4ClO_4$ propellant dec...
Heat-up times derived from studies on the ignition characteristics of a few model composite solid p...
Heat-up times derived from studies on the ignition characteristics of a few model composite solid pr...
Studies on the pyrolysis leading to ignition of polystyrene-$NH_4ClO_4$, PVC-$NH_4ClO_4$, and polyph...
Studies on the pyrolysis leading to ignition of polystyrene (PS)/ammonium perchlorate (AP), polyviny...
This paper describes a preliminary investigation into the effects of binder properties on composite ...
This is a first report in which the influence of the structure of polymeric binders, such as molecul...
This thesis document was issued under the authority of another institution, not NPS. At the time it...
Temperature profiles during polymerization, for the infinite solid cylinder, the infinite hollow cyl...
The role of thermal decomposition of the binder and the oxidiser in the thermal decomposition, agein...
Ignition of a composite aluminised propellant (AP-H1PB-A/) in stagnant hot air is analysed theoretic...
The role of thermal decomposition of the binder and the oxidiser in the thermal decomposition, agein...
Ignition of a composite aluminised propellant (AP-HTPB-Al) in stagnant hot air is analysed theoreti...
The propellant composition is one of several parameter that influencing the temperature sensitivity ...
Calorimetric value and ignition temp. of carboxy-terminated polybutadiene$/NH_4ClO_4$ propellant dec...
Heat-up times derived from studies on the ignition characteristics of a few model composite solid p...
Heat-up times derived from studies on the ignition characteristics of a few model composite solid pr...
Studies on the pyrolysis leading to ignition of polystyrene-$NH_4ClO_4$, PVC-$NH_4ClO_4$, and polyph...
Studies on the pyrolysis leading to ignition of polystyrene (PS)/ammonium perchlorate (AP), polyviny...
This paper describes a preliminary investigation into the effects of binder properties on composite ...
This is a first report in which the influence of the structure of polymeric binders, such as molecul...
This thesis document was issued under the authority of another institution, not NPS. At the time it...
Temperature profiles during polymerization, for the infinite solid cylinder, the infinite hollow cyl...
The role of thermal decomposition of the binder and the oxidiser in the thermal decomposition, agein...
Ignition of a composite aluminised propellant (AP-H1PB-A/) in stagnant hot air is analysed theoretic...
The role of thermal decomposition of the binder and the oxidiser in the thermal decomposition, agein...
Ignition of a composite aluminised propellant (AP-HTPB-Al) in stagnant hot air is analysed theoreti...
The propellant composition is one of several parameter that influencing the temperature sensitivity ...
Calorimetric value and ignition temp. of carboxy-terminated polybutadiene$/NH_4ClO_4$ propellant dec...