The local spatial heterogeneity of the material properties of the cortical and trabecular bone extracted from the mouse tibia is not well-known. Nevertheless, its characterization is fundamental to be able to study comprehensively the effect of interventions and to generate computational models to predict the bone strength preclinically. The goal of this study was to evaluate the nanoindentation properties of bone tissue extracted from two different mouse strains across the tibia length and in different sectors. Left tibiae were collected from four female mice, two C57BL/6, and two Balb/C mice. Nanoindentations with maximum 6 mN load were performed on different microstructures, regions along the axis of the tibiae, and sectors (379 in total...
Nanoindentation testing is a technique that is used to measure mechanical properties of materials at...
In this work, we demonstrate the viability of using our recently developed data analysis procedures ...
Bone is a strong and tough material composed of apatite mineral, organic matter, and water. Changes ...
The local spatial heterogeneity of the material properties of the cortical and trabecular bone extra...
Studies investigating micromechanical properties in mouse cortical bone often solely focus on the me...
Use of nanoindentation technology to identify quantitative trait loci (QTL) that regulate bone prope...
Studies investigating micromechanical properties in mouse cortical bone often solely focus on the me...
This PhD aimed at characterising mechanical, structural and compositional properties of cortical bo...
Understanding how bone adapts to mechanical stimuli is fundamental for optimising treatments against...
New treatments for bone diseases require testing in animal models before clinical translation, and t...
The mouse tibia is a common site to investigate bone remodelling and the effect of treatments precli...
Oestrogen deficiency-related bone loss in the ovariectomized (OVX) mouse is a common model for osteo...
Nanoindentation provides the ideal framework to determine mechanical properties of bone at the tissu...
Nanoindentation is widely used to measure the mechanical properties of bio-tissues. However, viscoel...
Nanoindentation provides the ideal framework to determine mechanical properties of bone at the tissu...
Nanoindentation testing is a technique that is used to measure mechanical properties of materials at...
In this work, we demonstrate the viability of using our recently developed data analysis procedures ...
Bone is a strong and tough material composed of apatite mineral, organic matter, and water. Changes ...
The local spatial heterogeneity of the material properties of the cortical and trabecular bone extra...
Studies investigating micromechanical properties in mouse cortical bone often solely focus on the me...
Use of nanoindentation technology to identify quantitative trait loci (QTL) that regulate bone prope...
Studies investigating micromechanical properties in mouse cortical bone often solely focus on the me...
This PhD aimed at characterising mechanical, structural and compositional properties of cortical bo...
Understanding how bone adapts to mechanical stimuli is fundamental for optimising treatments against...
New treatments for bone diseases require testing in animal models before clinical translation, and t...
The mouse tibia is a common site to investigate bone remodelling and the effect of treatments precli...
Oestrogen deficiency-related bone loss in the ovariectomized (OVX) mouse is a common model for osteo...
Nanoindentation provides the ideal framework to determine mechanical properties of bone at the tissu...
Nanoindentation is widely used to measure the mechanical properties of bio-tissues. However, viscoel...
Nanoindentation provides the ideal framework to determine mechanical properties of bone at the tissu...
Nanoindentation testing is a technique that is used to measure mechanical properties of materials at...
In this work, we demonstrate the viability of using our recently developed data analysis procedures ...
Bone is a strong and tough material composed of apatite mineral, organic matter, and water. Changes ...