A crystal plasticity finite element constitutive model combined with Bassani and Wu hardening law has been developed to investigate the effects of grain/phase boundary (GB/PB) on mechanical properties and microtexture evolution of Cu bicrystals and Cu–Al bicrystals during nanoindentation process. The simulated load–displacement curve for the Cu single crystal with Goss initial orientation has been analyzed and compared with the result from the experiment to validate the parameters. The numerical results indicate that the effects of GB/PB on load–displacement curves, indentation Young's moduli, Mises stresses, pile-up patterns are insignificant for Cu bicrystals while they are significant for Cu–Al bicrystals. The main reason is that PB work...
A three-dimensional crystal plasticity finite element method model is developed to investigate the i...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...
A crystal plasticity finite element method constitutive model was developed to investigate the aniso...
MasterThis thesis investigates deformation behaviors of Cu single crystals such as the indentation s...
Slip deformation in Cu-9 at.% Al symmetric type bicrystal models subjected to tensile loading is inv...
Slip deformation in Cu-9 at.% Al symmetric type bicrystal models subjected to tensile loading is inv...
Molecular dynamics (MD) simulations are performed to study crystalline plasticity during nanoindenta...
Molecular dynamics (MD) simulations are performed to study crystalline plasticity during nanoindenta...
International audienceThis work concerns analysis of Vickers and Berkovich indentation experiments t...
Abstract: Molecular dynamics (MD) simulations are performed to study crystalline plasticity during n...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...
A three-dimensional crystal plasticity finite element method model is developed to investigate the i...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...
A three-dimensional crystal plasticity finite element method model is developed to investigate the i...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...
A crystal plasticity finite element method constitutive model was developed to investigate the aniso...
MasterThis thesis investigates deformation behaviors of Cu single crystals such as the indentation s...
Slip deformation in Cu-9 at.% Al symmetric type bicrystal models subjected to tensile loading is inv...
Slip deformation in Cu-9 at.% Al symmetric type bicrystal models subjected to tensile loading is inv...
Molecular dynamics (MD) simulations are performed to study crystalline plasticity during nanoindenta...
Molecular dynamics (MD) simulations are performed to study crystalline plasticity during nanoindenta...
International audienceThis work concerns analysis of Vickers and Berkovich indentation experiments t...
Abstract: Molecular dynamics (MD) simulations are performed to study crystalline plasticity during n...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...
A three-dimensional crystal plasticity finite element method model is developed to investigate the i...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...
A three-dimensional crystal plasticity finite element method model is developed to investigate the i...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...
International audienceThe local mechanical behavior near symmetric tilt grain boundaries in aluminu...