Since the introduction of hot isostatic pressing (HIP) technology, it has been widely used in powder metallurgy forming and improving the densification of castings. With the increasing demand for the performance of nickel-based single crystal superalloy, more and more scholars started research on the application of hot isostatic pressing in nickel-based single crystal superalloy. This article summarizes the current research progress in the application of hot isostatic pressing to the high temperature of nickel-based single crystals, explains the elimination effect of hot isostatic pressing on porosity and other pore defects in nickel-based single crystal superalloy, analyzes the pore healing mechanism, and the changes in mechanical properti...
There the modelling technique of behaviour of microscopes at the annealing and after the Hot Isostat...
The effect of the hot oscillatory pressing (HOPing) temperature on the microstructure and tensile be...
An advanced powder metallurgy (P/M) nickel-base superalloy envisaged for aerospace applications is r...
Since the introduction of hot isostatic pressing (HIP) technology, it has been widely used in powder...
In this work, we investigate the effect of hot isostatic pressing on the intermediate temperature te...
Hot isostatic pressing (HIP) technology can effectively reduce microstructure defects such as microp...
Effects of the hot-isostatic pressing (HIP) temperature (1280,1300,1320℃) on microstructures and mec...
Pore annihilation was investigated in the single-crystal nickel-base superalloy CMSX-4. HIP tests at...
The microstructure of as-cast and as-HIPed (hot isostatic pressed) K403 superalloy was investigated ...
Hot isostatic pressing (HIP) is of interest to the aerospace industry due to the ability to produce ...
Hot Isostatic Pressing (HIP) is a powder metallurgy technique which densifies metallic powders via t...
For reducing the porosity of single crystal (SX) nickel-based superalloys, Hot Isostatic Pressing (H...
Under the typical hot isostatic pressing (HIP) processing conditions, plastic deformation by disloca...
Hot Isostatic Pressing (HIP) is a process that uniquely combines higher pressure and temperature to ...
In order to investigate the effect of hot isostatic pressing (HIP) process parameters on the propert...
There the modelling technique of behaviour of microscopes at the annealing and after the Hot Isostat...
The effect of the hot oscillatory pressing (HOPing) temperature on the microstructure and tensile be...
An advanced powder metallurgy (P/M) nickel-base superalloy envisaged for aerospace applications is r...
Since the introduction of hot isostatic pressing (HIP) technology, it has been widely used in powder...
In this work, we investigate the effect of hot isostatic pressing on the intermediate temperature te...
Hot isostatic pressing (HIP) technology can effectively reduce microstructure defects such as microp...
Effects of the hot-isostatic pressing (HIP) temperature (1280,1300,1320℃) on microstructures and mec...
Pore annihilation was investigated in the single-crystal nickel-base superalloy CMSX-4. HIP tests at...
The microstructure of as-cast and as-HIPed (hot isostatic pressed) K403 superalloy was investigated ...
Hot isostatic pressing (HIP) is of interest to the aerospace industry due to the ability to produce ...
Hot Isostatic Pressing (HIP) is a powder metallurgy technique which densifies metallic powders via t...
For reducing the porosity of single crystal (SX) nickel-based superalloys, Hot Isostatic Pressing (H...
Under the typical hot isostatic pressing (HIP) processing conditions, plastic deformation by disloca...
Hot Isostatic Pressing (HIP) is a process that uniquely combines higher pressure and temperature to ...
In order to investigate the effect of hot isostatic pressing (HIP) process parameters on the propert...
There the modelling technique of behaviour of microscopes at the annealing and after the Hot Isostat...
The effect of the hot oscillatory pressing (HOPing) temperature on the microstructure and tensile be...
An advanced powder metallurgy (P/M) nickel-base superalloy envisaged for aerospace applications is r...