Voltammetric and electrochemical impedance spectroscopic measurements in combination with ex situ surface analysis are used to characterise the passive state of Fe–18% Cr in molten NaOH at 470 °C. The areas of corrosion, passivity and transpassivity are derived from experimental voltammetric data and thermodynamic considerations. Impedance measurements in a wide potential range are performed to study the conductivity mechanism of the anodic layers formed. The surface composition of the passive film is estimated by X-ray photoelectron spectroscopy and its in-depth composition by Auger electron spectroscopy. A transfer function based on a tentative kinetic model is proposed to describe the impedance spectra. The parameters of the transfer fun...
The oxide films formed on AISI 316L(NG) in the temperature range 150-300°C in a simulated light wate...
The electrochemical behaviour of pure iron anodes in molten KHSO4 at 250°C was studied. Typical pass...
An examination has been carried out of the secondary passive film on Type 304 stainless steel in 0.5...
The passive state of three commercial highly alloyed austenitic stainless steels is studied by volta...
The characterisation of passive oxide films on heterogeneous microstructures is needed to assess loc...
International audienceThe passive films formed on laser-beam-melted (LBM) and conventional 17-4PH ma...
International audienceThe passivity and protective nature of the passive films are essentially relat...
A quantitative approach to evaluate the effect of the passive film on the corrosion resistance of fe...
Wide frequency range impedance measurements are applied to a kinetic investigation of passive iron i...
The passive state of Fe‐12% Cr and Fe‐25% Cr alloys in 1 M sulfate solutions of pH 0 and 5 was studi...
The behaviour of oxide films formed on Ni- and Fe-based alloys in different environments has been st...
The passivation and the transpassive dissolution of Fe–Cr alloys (12% and 25% Cr) was studied with a...
Passive films were grown at constant potential in acidic (pH∼2) and alkaline (pH∼13) solutions on ch...
This paper focuses on the characterisation of the electrochemical behaviour of a martensitic stainle...
The behavior of differently heat-treated X20Cr13 steels in 0.1 M H2SO4 was studied using the electro...
The oxide films formed on AISI 316L(NG) in the temperature range 150-300°C in a simulated light wate...
The electrochemical behaviour of pure iron anodes in molten KHSO4 at 250°C was studied. Typical pass...
An examination has been carried out of the secondary passive film on Type 304 stainless steel in 0.5...
The passive state of three commercial highly alloyed austenitic stainless steels is studied by volta...
The characterisation of passive oxide films on heterogeneous microstructures is needed to assess loc...
International audienceThe passive films formed on laser-beam-melted (LBM) and conventional 17-4PH ma...
International audienceThe passivity and protective nature of the passive films are essentially relat...
A quantitative approach to evaluate the effect of the passive film on the corrosion resistance of fe...
Wide frequency range impedance measurements are applied to a kinetic investigation of passive iron i...
The passive state of Fe‐12% Cr and Fe‐25% Cr alloys in 1 M sulfate solutions of pH 0 and 5 was studi...
The behaviour of oxide films formed on Ni- and Fe-based alloys in different environments has been st...
The passivation and the transpassive dissolution of Fe–Cr alloys (12% and 25% Cr) was studied with a...
Passive films were grown at constant potential in acidic (pH∼2) and alkaline (pH∼13) solutions on ch...
This paper focuses on the characterisation of the electrochemical behaviour of a martensitic stainle...
The behavior of differently heat-treated X20Cr13 steels in 0.1 M H2SO4 was studied using the electro...
The oxide films formed on AISI 316L(NG) in the temperature range 150-300°C in a simulated light wate...
The electrochemical behaviour of pure iron anodes in molten KHSO4 at 250°C was studied. Typical pass...
An examination has been carried out of the secondary passive film on Type 304 stainless steel in 0.5...