The magnetic and piezomagnetic properties of the strip-shaped samples of the Fe64Ni10Nb3Cu1Si13B9 alloy were investigated after annealing in vacuum in the temperature range 100–600 °C. The coercivity was in the range from 5 to 50 A/m, the saturation induction about 1.25 T and magnetostriction (22–26)×10−6 (after annealing up to 480 °C). The magnetomechanical coupling coefficient reached the value of 0.62, and the elasticity moduli were changing from 70 to 205 GPa
Among various soft magnetic materials, ferromagnetic glasses are superior to their crystalline count...
The microstructure and magnetic properties i.e. the initial permeability, magnetic after-effect and ...
The influence of a magnetic field upon magnetostriction and magnetomechanical coupling (k) was measu...
The magnetic and piezomagnetic properties of the strip-shaped samples of the Fe64Ni10Nb3Cu1Si13B9 al...
The piezomagnetic properties of rapidly quenched Fe73.5Cu1Nb3Si13.5B9 alloy strips were investigated...
The effect of different heat treatments on the piezomagnetic properties and magnetostriction of Fe73...
Magnetic field dependences of magnetomechanical coupling coefficient and moduli of elasticity in Fe7...
The magnetostriction and magnetomechanical coupling (k) in the Fe73.5Cu1Nb3Si13.5B9 strips annealed ...
The magnetostriction of Fe73.5CU1Nb3Si15.5B7 metallic glass, annealed in a vacuum for l h at tempera...
The effect of different heat treatments on the piezomagnetic properties and magnetostriction of Fe73...
Magnetostriction hysteresis loops of Fe73.5Cu1Nb3Si15.5B7 metallic glass strips annealed in vacuum f...
The magnetic and mechanical properties of amorphous ribbons heat treated in a conventional furnace a...
The magnetomechanical coupling coefficient (k) of amorphous Fe(73.5)Cu(1)Nb(3)Si1(5.5)B(7) alloy str...
In the present work, we study the influence of thermal treatments on the magnetic properties of as-q...
The Fe73.5Cu1Nb1Ta2Si13.5B9 samples were measured in as-quenched state and after annealing for 1 h i...
Among various soft magnetic materials, ferromagnetic glasses are superior to their crystalline count...
The microstructure and magnetic properties i.e. the initial permeability, magnetic after-effect and ...
The influence of a magnetic field upon magnetostriction and magnetomechanical coupling (k) was measu...
The magnetic and piezomagnetic properties of the strip-shaped samples of the Fe64Ni10Nb3Cu1Si13B9 al...
The piezomagnetic properties of rapidly quenched Fe73.5Cu1Nb3Si13.5B9 alloy strips were investigated...
The effect of different heat treatments on the piezomagnetic properties and magnetostriction of Fe73...
Magnetic field dependences of magnetomechanical coupling coefficient and moduli of elasticity in Fe7...
The magnetostriction and magnetomechanical coupling (k) in the Fe73.5Cu1Nb3Si13.5B9 strips annealed ...
The magnetostriction of Fe73.5CU1Nb3Si15.5B7 metallic glass, annealed in a vacuum for l h at tempera...
The effect of different heat treatments on the piezomagnetic properties and magnetostriction of Fe73...
Magnetostriction hysteresis loops of Fe73.5Cu1Nb3Si15.5B7 metallic glass strips annealed in vacuum f...
The magnetic and mechanical properties of amorphous ribbons heat treated in a conventional furnace a...
The magnetomechanical coupling coefficient (k) of amorphous Fe(73.5)Cu(1)Nb(3)Si1(5.5)B(7) alloy str...
In the present work, we study the influence of thermal treatments on the magnetic properties of as-q...
The Fe73.5Cu1Nb1Ta2Si13.5B9 samples were measured in as-quenched state and after annealing for 1 h i...
Among various soft magnetic materials, ferromagnetic glasses are superior to their crystalline count...
The microstructure and magnetic properties i.e. the initial permeability, magnetic after-effect and ...
The influence of a magnetic field upon magnetostriction and magnetomechanical coupling (k) was measu...