The aim of this research investigation was to study the long term effect of creep on different wood materials under natural environmental conditions. The tests were initiated in the summer of 1992 and the results collected until the end of 1995 are reported here. The experiments on sawn timber of pine and spruce, glulam, Kerto-LVL and I-profile with hardboard web structural size members were carried out in a sheltered environment, where the changes in moisture and temperature of the surrounding followed the natural climatic conditions of Southern Finland. In addition, separate tests on eight glulam beams were carried out in a heated room environment. The experiments were carried out at low load levels (2...7 MPa). The surface of few groups ...
A creep analysis has been performed on nailed, toothed-plates and split-ring joints in a varying unc...
The design of timber beams and joists is often governed by serviceability requirements, i.e., meetin...
Strength and stiffness of timber have been studied in different projects during 1986-2007. This is a...
The aim of this research investigation was to study the long term effect of creep on different wood ...
An experimental study on the creep of timber under low load levels, typical of long duration loads i...
An experimental study on the creep of timber under low load levels, typical of long duration loads i...
Graduation date: 1996In order to describe long term creep behavior of structural lumber in a natural...
An investigation was carried out to examine the effect of reinforcement on the creep behaviour of FR...
Two sets of data are analyzed in the thesis. The first set was derived from the long term deformatio...
Two sets of data are analyzed in the thesis. The first set was derived from the long term deformatio...
Timber is a natural material from matured trees that can be used for structural applications. Materi...
International audience-The main objective of this study is to know, the coupled impact of climatic v...
Strength and stiffness of timber have been studied in different projects during 1986-2007. This is a...
International audience-The main objective of this study is to know, the coupled impact of climatic v...
International audience-The main objective of this study is to know, the coupled impact of climatic v...
A creep analysis has been performed on nailed, toothed-plates and split-ring joints in a varying unc...
The design of timber beams and joists is often governed by serviceability requirements, i.e., meetin...
Strength and stiffness of timber have been studied in different projects during 1986-2007. This is a...
The aim of this research investigation was to study the long term effect of creep on different wood ...
An experimental study on the creep of timber under low load levels, typical of long duration loads i...
An experimental study on the creep of timber under low load levels, typical of long duration loads i...
Graduation date: 1996In order to describe long term creep behavior of structural lumber in a natural...
An investigation was carried out to examine the effect of reinforcement on the creep behaviour of FR...
Two sets of data are analyzed in the thesis. The first set was derived from the long term deformatio...
Two sets of data are analyzed in the thesis. The first set was derived from the long term deformatio...
Timber is a natural material from matured trees that can be used for structural applications. Materi...
International audience-The main objective of this study is to know, the coupled impact of climatic v...
Strength and stiffness of timber have been studied in different projects during 1986-2007. This is a...
International audience-The main objective of this study is to know, the coupled impact of climatic v...
International audience-The main objective of this study is to know, the coupled impact of climatic v...
A creep analysis has been performed on nailed, toothed-plates and split-ring joints in a varying unc...
The design of timber beams and joists is often governed by serviceability requirements, i.e., meetin...
Strength and stiffness of timber have been studied in different projects during 1986-2007. This is a...