The scanning reference electrode technique (SRET) has been used to examine corrosion in a galvanic ‘Kelocouple’ system, being that of an explosively bonded joint comprising a tri-metallic sandwich of steel/aluminium/aluminium alloy. Quantitative results of local current densities in 4% sea water at room temperature have been obtained. These have been compared with results from two conventional macroscopic techniques for measuring galvanic current, namely zero resistance ammetry and polarisation curves. The SRET results were found to be at least an order of magnitude higher than the average results obtained using the macroscopic methods. Comparison between SRET current densities and corrosion (as obtained by the amount of aluminium in soluti...
A new generation of lightweight subsea structures is planned for application in oil and gas producti...
The galvanic corrosion behavior of three metal alloys commonly used in water desalination plants was...
Galvanic corrosion on samples of AZ91D magnesium alloy coupled with 2A12 aluminum alloy during neutr...
The scanning reference electrode technique (SRET) has been used to examine corrosion in a galvanic '...
Instruments in the UK have pioneered the commercial development of a family of techniques which allo...
Many magnesium alloys exhibit microgalvanic corrosion due to anodic and cathodic reactions that occu...
At Forsmark, several cases of suspected galvanic corrosion have been detected and believed to be cau...
Galvanic corrosion behavior of A 516 steel separately coupled to six different corrosion-resistant a...
The local electrochemical properties of galvanic corrosion for three coupled metals in a desalinatio...
Galvanic corrosion behavior of A 516 steel coupled to alloy C-22 and Ti Gr-12, respectively was eval...
An investigation was carried out into the galvanic corrosion of magnesium alloy AZ91D in contact wit...
This thesis mainly concerns the development and application of a novel electrochemical method, based...
The subsea industry is moving its operations down onto the seabed. With this new direction in produc...
An increasing interest for use of aluminium in subsea structures has been seen the resent years, con...
Effective inhibition of a galvanic couple requires consideration of several factors. One factor is t...
A new generation of lightweight subsea structures is planned for application in oil and gas producti...
The galvanic corrosion behavior of three metal alloys commonly used in water desalination plants was...
Galvanic corrosion on samples of AZ91D magnesium alloy coupled with 2A12 aluminum alloy during neutr...
The scanning reference electrode technique (SRET) has been used to examine corrosion in a galvanic '...
Instruments in the UK have pioneered the commercial development of a family of techniques which allo...
Many magnesium alloys exhibit microgalvanic corrosion due to anodic and cathodic reactions that occu...
At Forsmark, several cases of suspected galvanic corrosion have been detected and believed to be cau...
Galvanic corrosion behavior of A 516 steel separately coupled to six different corrosion-resistant a...
The local electrochemical properties of galvanic corrosion for three coupled metals in a desalinatio...
Galvanic corrosion behavior of A 516 steel coupled to alloy C-22 and Ti Gr-12, respectively was eval...
An investigation was carried out into the galvanic corrosion of magnesium alloy AZ91D in contact wit...
This thesis mainly concerns the development and application of a novel electrochemical method, based...
The subsea industry is moving its operations down onto the seabed. With this new direction in produc...
An increasing interest for use of aluminium in subsea structures has been seen the resent years, con...
Effective inhibition of a galvanic couple requires consideration of several factors. One factor is t...
A new generation of lightweight subsea structures is planned for application in oil and gas producti...
The galvanic corrosion behavior of three metal alloys commonly used in water desalination plants was...
Galvanic corrosion on samples of AZ91D magnesium alloy coupled with 2A12 aluminum alloy during neutr...