The effects of cold deformation prior to aging on the precipitation behavior, microstructure and mechanical properties of an Al-5.6Cu-0.72 Mg-0.5Ag-0.32Mn-0.17Sc-0.12Zr (in wt%) alloy were investigated. Pre-straining disrupts the formation of Mg–Ag co-clusters, modifying the normal precipitation sequenc
The hardening and microstructural evolution during ageing of a Al-1.2Cu-0.5Mg and a Al-1.2Cu-1.2Mg (...
In this study, Al-1.00 Mg-0.65 Si-0.24 Cu alloy was solution heat-treated, water-quenched, and then ...
The precipitation behavior and aging response of an Al-4.9Cu-0.74Mg-0.51Si-0.48Mn-0.1Cr-0.08Ti-0.02F...
The effects of cold deformation prior to aging on the precipitation behavior, microstructure and mec...
The effects of 3%–50% pre-deformation following solution heat treatment on the age hardening of an A...
Pre-stretching prior to aging is known to degrade the performance of Al–Cu–Mg–Ag alloys at elevated ...
In this study, Al-1.00 Mg-0.65 Si-0.24 Cu alloy was solution heat-treated, water-quenched, and then ...
Effect of cold rolling prior to ageing on a dispersion of secondary phases and mechanical properties...
Effect of thermomechanical processing on creep resistance at 150°C of an Al-5.6Cu- 0.72Mg-0.5Ag-0.32...
This work presents a detailed investigation of the ageing behaviour of AA2519 alloy subjected to col...
A novel treatment process that involves solution treatment, cryogenic pre-stretching, and artificial...
Pre-rolling deformation is a preferable procedure in practice, compared to pre-stretching, to improv...
AbstractThe effect of increasing pre-stretching to higher levels, than are currently used in industr...
This work has investigated the effect of the combination of natural ageing and 80% pre-deformation a...
The effect of tensile strain ranging from 1% to 7% on the decomposition sequence and mechanical prop...
The hardening and microstructural evolution during ageing of a Al-1.2Cu-0.5Mg and a Al-1.2Cu-1.2Mg (...
In this study, Al-1.00 Mg-0.65 Si-0.24 Cu alloy was solution heat-treated, water-quenched, and then ...
The precipitation behavior and aging response of an Al-4.9Cu-0.74Mg-0.51Si-0.48Mn-0.1Cr-0.08Ti-0.02F...
The effects of cold deformation prior to aging on the precipitation behavior, microstructure and mec...
The effects of 3%–50% pre-deformation following solution heat treatment on the age hardening of an A...
Pre-stretching prior to aging is known to degrade the performance of Al–Cu–Mg–Ag alloys at elevated ...
In this study, Al-1.00 Mg-0.65 Si-0.24 Cu alloy was solution heat-treated, water-quenched, and then ...
Effect of cold rolling prior to ageing on a dispersion of secondary phases and mechanical properties...
Effect of thermomechanical processing on creep resistance at 150°C of an Al-5.6Cu- 0.72Mg-0.5Ag-0.32...
This work presents a detailed investigation of the ageing behaviour of AA2519 alloy subjected to col...
A novel treatment process that involves solution treatment, cryogenic pre-stretching, and artificial...
Pre-rolling deformation is a preferable procedure in practice, compared to pre-stretching, to improv...
AbstractThe effect of increasing pre-stretching to higher levels, than are currently used in industr...
This work has investigated the effect of the combination of natural ageing and 80% pre-deformation a...
The effect of tensile strain ranging from 1% to 7% on the decomposition sequence and mechanical prop...
The hardening and microstructural evolution during ageing of a Al-1.2Cu-0.5Mg and a Al-1.2Cu-1.2Mg (...
In this study, Al-1.00 Mg-0.65 Si-0.24 Cu alloy was solution heat-treated, water-quenched, and then ...
The precipitation behavior and aging response of an Al-4.9Cu-0.74Mg-0.51Si-0.48Mn-0.1Cr-0.08Ti-0.02F...