Nickel‐based single‐crystal superalloys are predominantly used for turbine blades in aircraft engines and land‐based gas turbines. Understanding and predicting the fatigue failure of Ni‐based single‐crystal superalloys are critical to ensure the safety of these components during operation. In this paper, low‐cycle fatigue experiments were carried out to investigate cyclic deformation of a nickel‐based single‐crystal superalloy MD2, recently developed by GE Power, with different crystallographic orientations. Specialty in situ scanning electron microscope (SEM) tests were also conducted to study the slip‐controlled initiation of short cracks under low‐cycle fatigue. In particular, the stress–strain response for both [001] and [111] orientati...
This dissertation expands upon the current knowledge of plastic deformation in nickel-based superall...
This work concerns the fatigue crack growth behaviour of nickel base single crystal superalloys. The...
AbstractSingle crystal (CMSX4) and oligocrystal (MAR002) nickel have been studied using three-point ...
Single-crystal nickel-based superalloys are dominantly used for turbine blades due to their superior...
In this dissertation the work done in the projects KME-410/502 will be presented.The overall objecti...
Cyclic deformation, oxidation damage and fatigue crack growth in nickel-based superalloys have ...
In this work stage I crack initiation in polycrystalline nickel-based superalloys is investigated by...
Low cycle fatigue is one of the main life limiting factors in gas turbine discs. The plastic deforma...
High-cycle fatigue-induced failures in turbine and turbopump blades is a pervasive problem. Single-c...
AbstractUsing crystal plasticity, finite element analyses were carried out to model cyclic deformati...
In this paper, cyclic plasticity in a single crystal nickel-based superalloy CMSX4 at elevated tempe...
The inherent anisotropy of single-crystal nickel-base superalloys brings many difficulties in terms ...
Fatigue crack growth was investigated in a 001 oriented single crystal specimen, made of a Ni-based ...
Using crystal plasticity, finite element analyses were carried out to model cyclic deformation for a...
Thanks to their excellent mechanical and chemical properties at temperatures up to 1000 °C, nickel-b...
This dissertation expands upon the current knowledge of plastic deformation in nickel-based superall...
This work concerns the fatigue crack growth behaviour of nickel base single crystal superalloys. The...
AbstractSingle crystal (CMSX4) and oligocrystal (MAR002) nickel have been studied using three-point ...
Single-crystal nickel-based superalloys are dominantly used for turbine blades due to their superior...
In this dissertation the work done in the projects KME-410/502 will be presented.The overall objecti...
Cyclic deformation, oxidation damage and fatigue crack growth in nickel-based superalloys have ...
In this work stage I crack initiation in polycrystalline nickel-based superalloys is investigated by...
Low cycle fatigue is one of the main life limiting factors in gas turbine discs. The plastic deforma...
High-cycle fatigue-induced failures in turbine and turbopump blades is a pervasive problem. Single-c...
AbstractUsing crystal plasticity, finite element analyses were carried out to model cyclic deformati...
In this paper, cyclic plasticity in a single crystal nickel-based superalloy CMSX4 at elevated tempe...
The inherent anisotropy of single-crystal nickel-base superalloys brings many difficulties in terms ...
Fatigue crack growth was investigated in a 001 oriented single crystal specimen, made of a Ni-based ...
Using crystal plasticity, finite element analyses were carried out to model cyclic deformation for a...
Thanks to their excellent mechanical and chemical properties at temperatures up to 1000 °C, nickel-b...
This dissertation expands upon the current knowledge of plastic deformation in nickel-based superall...
This work concerns the fatigue crack growth behaviour of nickel base single crystal superalloys. The...
AbstractSingle crystal (CMSX4) and oligocrystal (MAR002) nickel have been studied using three-point ...