A promising approach to deform metallic-intermetallic composite materials is the application of electric current pulses during the deformation process to achieve a lower yield strength and enhanced elongation to fracture. This is known as the electroplastic effect. In this work, a novel setup to study the electroplastic effect during nanoindentation on individual phases and well-defined interfaces was developed. Using a eutectic Al-Al2Cu alloy as a model material, electroplastic nanoindentation results were directly compared with macroscopic electroplastic compression tests. The results of the micro- and macroscopic investigations reveal current induced displacement shifts and stress drops, respectively, with the first displacement shift/st...
The objective of this research is twofold: first, to evaluate if the microscale Joule heating theory...
Application of electric pulses during plastic deformation of a metal results in reduction of flow st...
Increasingly strict fuel efficiency standards have driven the aerospace and automotive industries to...
A promising approach to deform metallic-intermetallic composite materials is the application of elec...
A promising approach to deform various groups of materials with poor deformability, such as metallic...
Application of high-intensity electric fields and/or currents is known to enhance materials’ deforma...
The electroplasticity phenomenon (EP) produces changes in the mechanical properties of a metal, due ...
학위논문 (박사)-- 서울대학교 대학원 : 재료공학부, 2016. 2. 한흥남.Electrically-assisted forming is a promising alternative...
The electro plastic effect (EPE) occurs in materials exposed to high electric currents, on the order...
Since the late 1950s, an effect of electrical current in addition to joule heating on the deformatio...
Metallic materials deform through discrete displacement bursts that are commonly associated with abr...
It is well known that increasing the temperature softens the materials and increases formability. Th...
The article deals with theoretical and experimental approaches to electroplastic deformation caused ...
Metallic materials play important roles in providing electrical, thermal, and mechanical functions i...
Manufacturing in automotive and aircraft industries are focused in improvement and cost reductions o...
The objective of this research is twofold: first, to evaluate if the microscale Joule heating theory...
Application of electric pulses during plastic deformation of a metal results in reduction of flow st...
Increasingly strict fuel efficiency standards have driven the aerospace and automotive industries to...
A promising approach to deform metallic-intermetallic composite materials is the application of elec...
A promising approach to deform various groups of materials with poor deformability, such as metallic...
Application of high-intensity electric fields and/or currents is known to enhance materials’ deforma...
The electroplasticity phenomenon (EP) produces changes in the mechanical properties of a metal, due ...
학위논문 (박사)-- 서울대학교 대학원 : 재료공학부, 2016. 2. 한흥남.Electrically-assisted forming is a promising alternative...
The electro plastic effect (EPE) occurs in materials exposed to high electric currents, on the order...
Since the late 1950s, an effect of electrical current in addition to joule heating on the deformatio...
Metallic materials deform through discrete displacement bursts that are commonly associated with abr...
It is well known that increasing the temperature softens the materials and increases formability. Th...
The article deals with theoretical and experimental approaches to electroplastic deformation caused ...
Metallic materials play important roles in providing electrical, thermal, and mechanical functions i...
Manufacturing in automotive and aircraft industries are focused in improvement and cost reductions o...
The objective of this research is twofold: first, to evaluate if the microscale Joule heating theory...
Application of electric pulses during plastic deformation of a metal results in reduction of flow st...
Increasingly strict fuel efficiency standards have driven the aerospace and automotive industries to...