© 2019 Elsevier LtdBeryllium oxide (BeO) thin films were grown on a p-type Si substrate by plasma enhanced atomic layer deposition (PEALD) using diethylberyllium as a precursor and O2 plasma. The PEALD BeO exhibited self-saturation and linear growth rates. The dielectric properties of PEALD were compared with those of thermal atomic layer deposition (ThALD). X-ray photoelectron spectroscopy was performed to determine the bandgap energy of PEALD BeO (8.0 eV) and ThALD BeO (7.9 eV). Capacitance–voltage curves revealed that PEALD BeO had low hysteresis and frequency dispersion compared to ThALD BeO. In addition, PEALD showed a dielectric constant of 7.15 (at 1 MHz) and low leakage current (7.25×10-9 A/cm2 at −1 MV/cm). These results indicate t...
Abstract—In a previous study, we demonstrated that the BeO film grown by atomic layer deposition (AL...
Silicon-on-insulator (SOI) technology improves the performance of devices by reducing parasitic capa...
The chemical and electrical characteristics of atomic layer deposited (ALD) beryllium oxide (BeO) on...
Beryllium oxide (BeO) thin films were grown on a p-type Si substrate by plasma enhanced atomic layer...
© 2021Beryllium oxide (BeO) is a unique metal oxide that exhibits high thermal conductivity and a hi...
In a previous study, atomic layer deposited (ALD) BeO exhibited less interface defect density and hy...
Beryllium oxide (BeO), which has excellent electrical insulating characteristics and high thermal st...
Growth characteristics and properties of BeO films grown by atomic layer deposition (ALD) are invest...
Growth characteristics and properties of BeO films grown by atomic layer deposition (ALD) are invest...
We report the energy-band alignment of atomic layer-deposited (ALD) beryllium oxide (BeO) films and ...
We report the energy-band alignment of atomic layer-deposited (ALD) beryllium oxide (BeO) films and ...
Beryllium oxide (BeO) is a promising dielectric because of its high energy bandgap (10.6 eV) and sho...
Electrical and physical characteristics of the atomic layer deposited beryllium oxide (BeO) grown on...
For the first time, an epitaxial beryllium oxide (BeO) film was grown on 4H silicon carbide (4H-SiC)...
We have grown a single-crystal beryllium oxide (BeO) thin film on a gallium nitride (GaN) substrate ...
Abstract—In a previous study, we demonstrated that the BeO film grown by atomic layer deposition (AL...
Silicon-on-insulator (SOI) technology improves the performance of devices by reducing parasitic capa...
The chemical and electrical characteristics of atomic layer deposited (ALD) beryllium oxide (BeO) on...
Beryllium oxide (BeO) thin films were grown on a p-type Si substrate by plasma enhanced atomic layer...
© 2021Beryllium oxide (BeO) is a unique metal oxide that exhibits high thermal conductivity and a hi...
In a previous study, atomic layer deposited (ALD) BeO exhibited less interface defect density and hy...
Beryllium oxide (BeO), which has excellent electrical insulating characteristics and high thermal st...
Growth characteristics and properties of BeO films grown by atomic layer deposition (ALD) are invest...
Growth characteristics and properties of BeO films grown by atomic layer deposition (ALD) are invest...
We report the energy-band alignment of atomic layer-deposited (ALD) beryllium oxide (BeO) films and ...
We report the energy-band alignment of atomic layer-deposited (ALD) beryllium oxide (BeO) films and ...
Beryllium oxide (BeO) is a promising dielectric because of its high energy bandgap (10.6 eV) and sho...
Electrical and physical characteristics of the atomic layer deposited beryllium oxide (BeO) grown on...
For the first time, an epitaxial beryllium oxide (BeO) film was grown on 4H silicon carbide (4H-SiC)...
We have grown a single-crystal beryllium oxide (BeO) thin film on a gallium nitride (GaN) substrate ...
Abstract—In a previous study, we demonstrated that the BeO film grown by atomic layer deposition (AL...
Silicon-on-insulator (SOI) technology improves the performance of devices by reducing parasitic capa...
The chemical and electrical characteristics of atomic layer deposited (ALD) beryllium oxide (BeO) on...