Study of glass transition kinetics of As2S3 and As2Se3 by ultrafast differential scanning calorimetr
The kinetics of crystallization of Pb15Ge27Se58 was studied by differential scanning calorimetry non...
Thermal behavior of chalcogen additive materials synthesized via melt quench method can be studied b...
Differential scanning calorimetry (DSC) can be used for obtaining various non-isothermal properties ...
Enthalpic relaxation was investigated on the As2Se3 bulk glass with perfectly defined thermal histor...
Differential scanning calorimetry (DSC) was performed at different heating rates under non-isotherma...
Glaiis transitions of As-Se glasses have been investigated over a wide range of compositions by usin...
Differential scanning calorimetry (DSC) measurements were performed at different heating rates under...
Bulk As–Te–In glasses have been prepared by conventional melt-quenching technique. Modulated differe...
A newly derived crystallization kinetics equation was presented for investigation on crystallization...
Results of thermal analysis performed at different heating rates on eight glasses of the As-Sb-Se sy...
Differential scanning calorimetry measurements under non-isothermal conditions were performed on the...
Reversible amorphous–crystalline phase transitions are studied using complementary ultrafast differe...
International audienceIn the present work, thermal properties of GeSe2-As2Se3-CdSe glasses were inve...
Fysische en Chemische MetaalkundeTechnische MateriaalwetenschappenApplied Science
International audienceThis work focuses on the study of the physical aging of a selenium glass by di...
The kinetics of crystallization of Pb15Ge27Se58 was studied by differential scanning calorimetry non...
Thermal behavior of chalcogen additive materials synthesized via melt quench method can be studied b...
Differential scanning calorimetry (DSC) can be used for obtaining various non-isothermal properties ...
Enthalpic relaxation was investigated on the As2Se3 bulk glass with perfectly defined thermal histor...
Differential scanning calorimetry (DSC) was performed at different heating rates under non-isotherma...
Glaiis transitions of As-Se glasses have been investigated over a wide range of compositions by usin...
Differential scanning calorimetry (DSC) measurements were performed at different heating rates under...
Bulk As–Te–In glasses have been prepared by conventional melt-quenching technique. Modulated differe...
A newly derived crystallization kinetics equation was presented for investigation on crystallization...
Results of thermal analysis performed at different heating rates on eight glasses of the As-Sb-Se sy...
Differential scanning calorimetry measurements under non-isothermal conditions were performed on the...
Reversible amorphous–crystalline phase transitions are studied using complementary ultrafast differe...
International audienceIn the present work, thermal properties of GeSe2-As2Se3-CdSe glasses were inve...
Fysische en Chemische MetaalkundeTechnische MateriaalwetenschappenApplied Science
International audienceThis work focuses on the study of the physical aging of a selenium glass by di...
The kinetics of crystallization of Pb15Ge27Se58 was studied by differential scanning calorimetry non...
Thermal behavior of chalcogen additive materials synthesized via melt quench method can be studied b...
Differential scanning calorimetry (DSC) can be used for obtaining various non-isothermal properties ...