The microstructure and mechanical properties of Fe-18Mn-0.6C and Fe-18Mn-0.4C steels subjected to rolling with a total reduction of 60% at temperatures of 773 K to 1373 K were investigate
A novel medium manganese steel with composition Fe–8.3Mn–3.8Al–1.8Si–0.5C–0.06V–0.05Sn was developed...
High Mn steels, alloyed with Si and Al, present large plasticity when deformed due to the TRIP/TWIP ...
In the paper, two grades of high-manganese steels with aluminum after a thermos - mechanical treatme...
The mechanical properties of medium to high-Mn austenitic TWIP/TRIP steels subjected to warm to hot ...
The microstructure and mechanical properties of Fe-18Mn-0.6C and Fe-18Mn-0.4C steels subjected to ro...
The structure-property relationship was studied in an Fe-18Mn-0.6C-1.5Al steel subjected to cold rol...
The influence of rolling at 77 K and 293 K to a true strain of 2.66 on the microstructure and textur...
The effects of rolling temperature ranging from −55 to 300 °C on dislocation density, twinning behav...
The microstructure and texture evolution during cold rolling with total thickness reductions of 20-8...
The deformation behavior of 18%Mn TWIP steels (upon tensile tests) subjected to warm-to-hot rolling ...
The structure–property relationship was studied in an Fe-18Mn-0.6C-1.5Al steel subjected to cold rol...
The effects of warm rolling reduction ratio ranging from 20% to 55% on microstructure evolution, the...
The microstructure and mechanical properties of cold-rolled Fe-18Mn-3Al-3Si-0.03C transformation ind...
This study investigated the microstructure and mechanical properties of hot-rolled and cold-rolled m...
Effect of cold rolling on the microstructure and mechanical properties of a Fe-23Mn- 0.3C-1.5Al (in ...
A novel medium manganese steel with composition Fe–8.3Mn–3.8Al–1.8Si–0.5C–0.06V–0.05Sn was developed...
High Mn steels, alloyed with Si and Al, present large plasticity when deformed due to the TRIP/TWIP ...
In the paper, two grades of high-manganese steels with aluminum after a thermos - mechanical treatme...
The mechanical properties of medium to high-Mn austenitic TWIP/TRIP steels subjected to warm to hot ...
The microstructure and mechanical properties of Fe-18Mn-0.6C and Fe-18Mn-0.4C steels subjected to ro...
The structure-property relationship was studied in an Fe-18Mn-0.6C-1.5Al steel subjected to cold rol...
The influence of rolling at 77 K and 293 K to a true strain of 2.66 on the microstructure and textur...
The effects of rolling temperature ranging from −55 to 300 °C on dislocation density, twinning behav...
The microstructure and texture evolution during cold rolling with total thickness reductions of 20-8...
The deformation behavior of 18%Mn TWIP steels (upon tensile tests) subjected to warm-to-hot rolling ...
The structure–property relationship was studied in an Fe-18Mn-0.6C-1.5Al steel subjected to cold rol...
The effects of warm rolling reduction ratio ranging from 20% to 55% on microstructure evolution, the...
The microstructure and mechanical properties of cold-rolled Fe-18Mn-3Al-3Si-0.03C transformation ind...
This study investigated the microstructure and mechanical properties of hot-rolled and cold-rolled m...
Effect of cold rolling on the microstructure and mechanical properties of a Fe-23Mn- 0.3C-1.5Al (in ...
A novel medium manganese steel with composition Fe–8.3Mn–3.8Al–1.8Si–0.5C–0.06V–0.05Sn was developed...
High Mn steels, alloyed with Si and Al, present large plasticity when deformed due to the TRIP/TWIP ...
In the paper, two grades of high-manganese steels with aluminum after a thermos - mechanical treatme...