The blends of poly(trimethylene terephthalate) (PTT) and ethylene propylene diene monomer (EPDM) with different composition have been studied by positron lifetime technique (PLT) and differential scanning calorimetric (DSC) measurements. The DSC results for the blends of 50/50 and 40/60 show clear two glass transition temperatures indicating two-phase system. No melting point depression was observed for the blend system, which strongly supports the incompatibility. From the positron results an increase in free volume hole size and its concentration has been observed with the increase in EPDM content of the blend which indicates further that there is coalescence of free volumes of EPDM with the PTT to some extent and phase separation behavio...
A method including cryogenic grinding, melt pressing from the molten state, and quenching was used t...
Phase behavior and its effects on crystallization in an extruded poly(trimethylene terephthalate) (P...
The chemical heterogeneity of poly(ethylene terephthalate) (PET) and of poly(ethylene terephthalate-...
The blends of poly(trimethylene terephthalate) (PTT) and ethylene propylene diene monomer (EPDM) wit...
Abstract Blends of poly(trimethylene terephthalate) (PTT) and ethylene propylene diene monomer (EPDM...
Abstract Differential scanning calorimetry (DSC) and positron annihilation lifetime measurements hav...
Positron lifetimes in polypropylene/ethylene-propylene-diene monomer blend (PP/EPDM, EPDM volume con...
A new method to characterize individual interfaces in ternary polymer blends from experimentally mea...
The morphology of immiscible and highly incompatible blends of Sorona(R) polymer Poly(trimethylene t...
The free volume of a polymer, which corresponds to the unoccupied regions accessible to segmental mo...
The aim of this study was to develop radiation sterilized polypropylene/ethylene-propylene diene mon...
The structural defects of linear low density polyethylene (LLDPE) and high density polyethylene (HOP...
Positron Annihilation Lifetime Spectroscopy has been used to determine the free volume content in th...
Polymer blends are a versatile playground for studying phase separation and its effect on the develo...
Miscibility and phase separation behaviour in blends of isotactic polypropylene (iPP) and ethylene-p...
A method including cryogenic grinding, melt pressing from the molten state, and quenching was used t...
Phase behavior and its effects on crystallization in an extruded poly(trimethylene terephthalate) (P...
The chemical heterogeneity of poly(ethylene terephthalate) (PET) and of poly(ethylene terephthalate-...
The blends of poly(trimethylene terephthalate) (PTT) and ethylene propylene diene monomer (EPDM) wit...
Abstract Blends of poly(trimethylene terephthalate) (PTT) and ethylene propylene diene monomer (EPDM...
Abstract Differential scanning calorimetry (DSC) and positron annihilation lifetime measurements hav...
Positron lifetimes in polypropylene/ethylene-propylene-diene monomer blend (PP/EPDM, EPDM volume con...
A new method to characterize individual interfaces in ternary polymer blends from experimentally mea...
The morphology of immiscible and highly incompatible blends of Sorona(R) polymer Poly(trimethylene t...
The free volume of a polymer, which corresponds to the unoccupied regions accessible to segmental mo...
The aim of this study was to develop radiation sterilized polypropylene/ethylene-propylene diene mon...
The structural defects of linear low density polyethylene (LLDPE) and high density polyethylene (HOP...
Positron Annihilation Lifetime Spectroscopy has been used to determine the free volume content in th...
Polymer blends are a versatile playground for studying phase separation and its effect on the develo...
Miscibility and phase separation behaviour in blends of isotactic polypropylene (iPP) and ethylene-p...
A method including cryogenic grinding, melt pressing from the molten state, and quenching was used t...
Phase behavior and its effects on crystallization in an extruded poly(trimethylene terephthalate) (P...
The chemical heterogeneity of poly(ethylene terephthalate) (PET) and of poly(ethylene terephthalate-...