Thin films were thermally evaporated from the bulk glasses of As40Se60−xSbx (with x=0, 5, 10, 15at.) under high vacuum. We have characterized the deposited films by Fourier Transform Infrared spectroscopy. The relationship between the structural and optical properties and the compositional variation has been investigated. Increasing Sb content was found to affect the thermal and optical properties of these films. Non-direct electronic transition was found to be responsible for the photon absorption inside the investigated films. It was found that, the optical band gap Eo decreases while the width of localized states (Urbach energy) Ee increases
In this paper we report results from studying changes in the optical properties of thin vacuum depos...
The thermally evaporated As20Sb20S60 amorphous film of 800 nm thickness was subjected to light expos...
The thermally evaporated As20Sb20S60 amorphous film of 800 nm thickness was subjected to light expos...
Thin films were thermally evaporated from the bulk glasses of As40Se60-xSbx (with x = 0, 5, 10, 15 a...
Thin films of SbxSe60-xS40( x= 10, 20, 30, and 40) were deposited by thermal evaporation from the pr...
Thin films of SbxSe60-xS40( x= 10, 20, 30, and 40) were deposited by thermal evaporation from the pr...
Thin films of Sb40Se20S40 with thickness 1000 nm were prepared by thermal evaporation technique. The...
Thin films of Sb20S40Se40 of thickness 800 nm were prepared by thermal evaporation method. The as-pr...
Thin films of Sb20S40Se40 of thickness 800 nm were prepared by thermal evaporation method. The as-pr...
Bulk samples of S40Se60,Sb-x (with x=10, 20, 30 and 40 at. %) were prepared from high purity chemica...
Bulk samples of S40Se60,Sb-x (with x=10, 20, 30 and 40 at. %) were prepared from high purity chemica...
Chalcogenide glasses are interesting materials for their infrared transmitting properties and photo-...
Chalcogenide glasses are interesting materials for their infrared transmitting properties and photo-...
The exposure with band gap light of thermally evaporated As40Sb15Se45 amorphous film of 800 nm thick...
GexSb40-xSe60 (where 10≤ x≤ 30 at %) thin films were prepared on glass substrates by thermal evapora...
In this paper we report results from studying changes in the optical properties of thin vacuum depos...
The thermally evaporated As20Sb20S60 amorphous film of 800 nm thickness was subjected to light expos...
The thermally evaporated As20Sb20S60 amorphous film of 800 nm thickness was subjected to light expos...
Thin films were thermally evaporated from the bulk glasses of As40Se60-xSbx (with x = 0, 5, 10, 15 a...
Thin films of SbxSe60-xS40( x= 10, 20, 30, and 40) were deposited by thermal evaporation from the pr...
Thin films of SbxSe60-xS40( x= 10, 20, 30, and 40) were deposited by thermal evaporation from the pr...
Thin films of Sb40Se20S40 with thickness 1000 nm were prepared by thermal evaporation technique. The...
Thin films of Sb20S40Se40 of thickness 800 nm were prepared by thermal evaporation method. The as-pr...
Thin films of Sb20S40Se40 of thickness 800 nm were prepared by thermal evaporation method. The as-pr...
Bulk samples of S40Se60,Sb-x (with x=10, 20, 30 and 40 at. %) were prepared from high purity chemica...
Bulk samples of S40Se60,Sb-x (with x=10, 20, 30 and 40 at. %) were prepared from high purity chemica...
Chalcogenide glasses are interesting materials for their infrared transmitting properties and photo-...
Chalcogenide glasses are interesting materials for their infrared transmitting properties and photo-...
The exposure with band gap light of thermally evaporated As40Sb15Se45 amorphous film of 800 nm thick...
GexSb40-xSe60 (where 10≤ x≤ 30 at %) thin films were prepared on glass substrates by thermal evapora...
In this paper we report results from studying changes in the optical properties of thin vacuum depos...
The thermally evaporated As20Sb20S60 amorphous film of 800 nm thickness was subjected to light expos...
The thermally evaporated As20Sb20S60 amorphous film of 800 nm thickness was subjected to light expos...