The thermal properties and heat-induced denaturation and aggregation of soy protein isolates (SPI) were studied using modulated differential scanning calorimetry (MDSC). Reversible and non-reversible heat flow signals were separated from the total heat flow signals in the thermograms. In the non-reversible profiles, two major endothermic peaks (at around 100 and 220 °C, respectively) associated with the loss of residual water were identified. In the reversible profiles, an exothermic peak associated with thermal aggregation was observed. Soy proteins denatured to various extents by heat treatments showed different non-reversible and reversible heat flow patterns, especially the exothermic peak. The endothermic or exothermic transition chara...
<p>key words: soy protein; glycinin; thermal stability; pH; ionic strength;genetic variant; so...
Previous work has shown that following the inclusion of alginate high in mannuronic acid there is a ...
In this study, we investigated the effect of isochoric moisture heating on the functionalities of si...
The thermal properties and heat-induced denaturation and aggregation of soy protein isolates (SPI) w...
Hydration properties of soybean isolates with different processing conditions (heat treatments, pH a...
Heat-induced gel formation by soy protein isolate at pH 7 is discussed. Different heating and coolin...
The aim of this work was to analyze the possible use of differential scanning calorimetry (DSC) as a...
<strong>Keywords:</strong> soy protein isolate, glycinin,β-conglycinin, heat denaturation, gelation,...
Keywords: soy protein isolate, glycinin,β-conglycinin, heat denaturation, gelation, network structur...
key words: soy protein; glycinin; thermal stability; pH; ionic strength;genetic variant; solubility;...
The objective of this thesis was to study the effect of heat treatment and glycation on five industr...
Vacuum and temperature effects on moisture content, water vapor permeability (WVP), color (L, a, b, ...
The effect of storage temperature on the physicochemical characteristics, solubility and gelling pro...
This paper provides a systematic study of the impact of different thermal treatments (62 ± 2°C, with...
Dry and subsequent wet heating were used to glycate soy proteins with dextran or glucose, followed b...
<p>key words: soy protein; glycinin; thermal stability; pH; ionic strength;genetic variant; so...
Previous work has shown that following the inclusion of alginate high in mannuronic acid there is a ...
In this study, we investigated the effect of isochoric moisture heating on the functionalities of si...
The thermal properties and heat-induced denaturation and aggregation of soy protein isolates (SPI) w...
Hydration properties of soybean isolates with different processing conditions (heat treatments, pH a...
Heat-induced gel formation by soy protein isolate at pH 7 is discussed. Different heating and coolin...
The aim of this work was to analyze the possible use of differential scanning calorimetry (DSC) as a...
<strong>Keywords:</strong> soy protein isolate, glycinin,β-conglycinin, heat denaturation, gelation,...
Keywords: soy protein isolate, glycinin,β-conglycinin, heat denaturation, gelation, network structur...
key words: soy protein; glycinin; thermal stability; pH; ionic strength;genetic variant; solubility;...
The objective of this thesis was to study the effect of heat treatment and glycation on five industr...
Vacuum and temperature effects on moisture content, water vapor permeability (WVP), color (L, a, b, ...
The effect of storage temperature on the physicochemical characteristics, solubility and gelling pro...
This paper provides a systematic study of the impact of different thermal treatments (62 ± 2°C, with...
Dry and subsequent wet heating were used to glycate soy proteins with dextran or glucose, followed b...
<p>key words: soy protein; glycinin; thermal stability; pH; ionic strength;genetic variant; so...
Previous work has shown that following the inclusion of alginate high in mannuronic acid there is a ...
In this study, we investigated the effect of isochoric moisture heating on the functionalities of si...