Porcelain compositions were prepared with and without the addition of mineralizers/nucleating agents and their phase assemblages were studied before and after subjecting them to heat-treatment. Mullite, quartz and glass were defected in the compositions before hear-treatment, but cristobalite appeared as an additional phase after heat-treatment. Heat-treated compositions were comparatively rich in mullite following crystallization from the glassy phase. Nb2O5 was the most efficient nucleating agent among those tried
A high sintering temperature is required to acquire excellent performance in the production of porce...
Titania was progressively added in the range 3-9 wt% into a triaxial porcelain body consisting of cl...
China clay (kaolin) was progressively replaced by pyrophyllite in a conventional porcelain mix. Addi...
Porcelain samples were prepared with and without the addition of mineralizers. The samples were then...
The phase and microstructure changes in two porcelain bodies as they evolve during firing were inves...
China clay (Kaolin) and quartz in the ratio of 1:2 was progressively replaced by pyrophyllite in a c...
In the present investigation, three quartz-free porcelain compositions were prepared where quartz wa...
The effect of alkali-silicate glassy matrix as replacement for feldspar in soft and hard porcelain c...
Ceramic raw materials from High Latium (Central Italy) consisting of halloysite-10 Å, amorphous sili...
The effect of alkali-silicate glassy matrix as replacement for feldspar in soft and hard porcelain c...
Porcelain bodies fabricated from triaxial mixtures of clay, quartz and feldspar with different amoun...
Feldspar was gradually substituted by B.F. slag (a glassy by-product of Indian steel plant) to the e...
Both quartz and feldspar were progressively replaced by ground sillimanite sand and glass-ceramics i...
A high sintering temperature is required to acquire excellent performance in the production of porce...
Pressed compacts of an industrial spray-dried porcelain stoneware powder, consisting mainly of albit...
A high sintering temperature is required to acquire excellent performance in the production of porce...
Titania was progressively added in the range 3-9 wt% into a triaxial porcelain body consisting of cl...
China clay (kaolin) was progressively replaced by pyrophyllite in a conventional porcelain mix. Addi...
Porcelain samples were prepared with and without the addition of mineralizers. The samples were then...
The phase and microstructure changes in two porcelain bodies as they evolve during firing were inves...
China clay (Kaolin) and quartz in the ratio of 1:2 was progressively replaced by pyrophyllite in a c...
In the present investigation, three quartz-free porcelain compositions were prepared where quartz wa...
The effect of alkali-silicate glassy matrix as replacement for feldspar in soft and hard porcelain c...
Ceramic raw materials from High Latium (Central Italy) consisting of halloysite-10 Å, amorphous sili...
The effect of alkali-silicate glassy matrix as replacement for feldspar in soft and hard porcelain c...
Porcelain bodies fabricated from triaxial mixtures of clay, quartz and feldspar with different amoun...
Feldspar was gradually substituted by B.F. slag (a glassy by-product of Indian steel plant) to the e...
Both quartz and feldspar were progressively replaced by ground sillimanite sand and glass-ceramics i...
A high sintering temperature is required to acquire excellent performance in the production of porce...
Pressed compacts of an industrial spray-dried porcelain stoneware powder, consisting mainly of albit...
A high sintering temperature is required to acquire excellent performance in the production of porce...
Titania was progressively added in the range 3-9 wt% into a triaxial porcelain body consisting of cl...
China clay (kaolin) was progressively replaced by pyrophyllite in a conventional porcelain mix. Addi...