International audienceThe mechanical behavior of the cortical bone in nanoindentation is a complicated mechanical problem. The finite element analysis has commonly been assumed to be the most appropriate approach to this issue. One significant problem in nanoindentation modeling of the elastic-plastic materials is pileup deformation, which is not observed in cortical bone nanoindentation testing. This phenomenon depends on the work-hardening of materials; it doesn't occur for work-hardening materials, which suggests that the cor-tical bone could be considered as a work-hardening material. Furthermore, in a recent study [59], a plastic hardening until failure was observed on the micro-scale of a dry ovine osteonal bone samples subjected to m...
A visco-elasto-plastic constitutive model is formulated for investigating the mechanics of cortical ...
Bone encompasses a complex arrangement of materials at different length scales, which endows it with...
Computer-aided methods such as finite-element simulation offer a great potential in the forensic rec...
International audienceThe mechanical behavior of the cortical bone in nanoindentation is a complicat...
Anisotropy is one of the most peculiar aspects of cortical bone mechanical behaviour, and the numeri...
In this work, a finite element model was developed for the numerical simulation of nanoindentation t...
The aim of this paper is to show that damage mechanisms can account for the response of lamellar bon...
Nanoindentation is a useful technique for probing the mechanical properties of bone, and finite elem...
A mechanical behaviour of bone tissues is defined by mechanical properties of its microstructural co...
Division of Biomechanics participates in a project together with Department of Cancer Research and M...
Evaluating the mechanical response of bone under high loading rates is crucial to understanding frac...
The purpose of this study is to investigate the effect of anisotropy of cortical bone tissue on meas...
Bone tissue is a material with a complex structure and mechanical properties. Diseases or even norma...
Bone-fracture susceptibility is increased by factors such as bone loss, microstructure changes, and ...
Prevention and treatment of osteoporosis rely on understanding of the micromechanical behaviour of b...
A visco-elasto-plastic constitutive model is formulated for investigating the mechanics of cortical ...
Bone encompasses a complex arrangement of materials at different length scales, which endows it with...
Computer-aided methods such as finite-element simulation offer a great potential in the forensic rec...
International audienceThe mechanical behavior of the cortical bone in nanoindentation is a complicat...
Anisotropy is one of the most peculiar aspects of cortical bone mechanical behaviour, and the numeri...
In this work, a finite element model was developed for the numerical simulation of nanoindentation t...
The aim of this paper is to show that damage mechanisms can account for the response of lamellar bon...
Nanoindentation is a useful technique for probing the mechanical properties of bone, and finite elem...
A mechanical behaviour of bone tissues is defined by mechanical properties of its microstructural co...
Division of Biomechanics participates in a project together with Department of Cancer Research and M...
Evaluating the mechanical response of bone under high loading rates is crucial to understanding frac...
The purpose of this study is to investigate the effect of anisotropy of cortical bone tissue on meas...
Bone tissue is a material with a complex structure and mechanical properties. Diseases or even norma...
Bone-fracture susceptibility is increased by factors such as bone loss, microstructure changes, and ...
Prevention and treatment of osteoporosis rely on understanding of the micromechanical behaviour of b...
A visco-elasto-plastic constitutive model is formulated for investigating the mechanics of cortical ...
Bone encompasses a complex arrangement of materials at different length scales, which endows it with...
Computer-aided methods such as finite-element simulation offer a great potential in the forensic rec...