Erbium doped tellurite glasses (TPE), having composition (70TeO(2)-(30 - x)ZnO-xPbO)(0.99)-(Er2O3)(0.01) (x = 5, 10, 15, and 20), were prepared by melt quenching technique and characterized by density measurements, Raman and optical spectroscopies and extended X-ray absorption fine structure (EXAFS) experiments. The main structural modifications of glasses as a function of the PbO/ZnO ratio are monitored by Raman scattering. EXAFS analysis shows almost unchanged short range environment around Er3+ ions for all glasses. Absorption and luminescence spectra evidence a significant decrease of the asymmetry of crystal field at the Er3+ ion site as the PbO content increases. (C) 2013 Elsevier B.V. All rights reserved
Er2O3-doped TeO2-ZnO-La2O3 modified tellurite glasses were prepared by the conventional melt-quenchi...
Er3+ doped tellurite glasses of molar composition (80-x)TeO2-18ZnO-1MgO-1Li2O-(x)Er2O3 system (0.5mo...
Series of Er3+ doped tellurite glass of the TeO2-PbO-Li2O-Nd2O3-Er2O3 system was successfully been m...
Erbium activated PbO-ZnO tellurite glasses ((70TeO(2)-(30 - x)ZnO-xPbO)(0.99)-(Er2O3)(0.01) (TZPE), ...
We present a comparison of the local structure of erbium in zinc-lead tellurite glasses and in silic...
Erbium zinc borotellurite, {[(TeO2)0.70(B2O3)0.30]0.7 (ZnO)0.3}1-y (Er3O2)y glasses were prepared by...
Erbium zinc borotellurite, {[(TeO2)0.70(B2O3)0.30]0.7 (ZnO)0.3}1-y (Er3O2)y glasses were prepared by...
Erbium zinc borotellurite, {[(TeO2)0.70(B2O3)0.30]0.7 (ZnO)0.3}1-y (Er3O2)y glasses were prepared by...
Understanding the influence of rare earth ions in improving the structural and optical properties of...
In this research, the melt-quenching method was used to synthesize a series of zinc tellurite glass ...
In this research, the melt-quenching method was used to synthesize a series of zinc tellurite glass ...
Structural, thermal and optical properties of lead-tellurite oxide glasses consisting TeO2 – PbO – B...
Er3+-doped tellurite glasses with molar compositions of xEr2O3-20ZnO-(80-x)TeO2 (x=0, 1, 2, 3, and 4...
Er3+-doped tellurite glasses with molar compositions of xEr2O3-20ZnO-(80 - x)TeO2 (x = 0, 1, 2, 3, a...
Er 3+ doped tellurite glasses of molar composition (80-x)TeO2-18ZnO-1MgO-1Li2O- (x)Er2O3 system (0.5...
Er2O3-doped TeO2-ZnO-La2O3 modified tellurite glasses were prepared by the conventional melt-quenchi...
Er3+ doped tellurite glasses of molar composition (80-x)TeO2-18ZnO-1MgO-1Li2O-(x)Er2O3 system (0.5mo...
Series of Er3+ doped tellurite glass of the TeO2-PbO-Li2O-Nd2O3-Er2O3 system was successfully been m...
Erbium activated PbO-ZnO tellurite glasses ((70TeO(2)-(30 - x)ZnO-xPbO)(0.99)-(Er2O3)(0.01) (TZPE), ...
We present a comparison of the local structure of erbium in zinc-lead tellurite glasses and in silic...
Erbium zinc borotellurite, {[(TeO2)0.70(B2O3)0.30]0.7 (ZnO)0.3}1-y (Er3O2)y glasses were prepared by...
Erbium zinc borotellurite, {[(TeO2)0.70(B2O3)0.30]0.7 (ZnO)0.3}1-y (Er3O2)y glasses were prepared by...
Erbium zinc borotellurite, {[(TeO2)0.70(B2O3)0.30]0.7 (ZnO)0.3}1-y (Er3O2)y glasses were prepared by...
Understanding the influence of rare earth ions in improving the structural and optical properties of...
In this research, the melt-quenching method was used to synthesize a series of zinc tellurite glass ...
In this research, the melt-quenching method was used to synthesize a series of zinc tellurite glass ...
Structural, thermal and optical properties of lead-tellurite oxide glasses consisting TeO2 – PbO – B...
Er3+-doped tellurite glasses with molar compositions of xEr2O3-20ZnO-(80-x)TeO2 (x=0, 1, 2, 3, and 4...
Er3+-doped tellurite glasses with molar compositions of xEr2O3-20ZnO-(80 - x)TeO2 (x = 0, 1, 2, 3, a...
Er 3+ doped tellurite glasses of molar composition (80-x)TeO2-18ZnO-1MgO-1Li2O- (x)Er2O3 system (0.5...
Er2O3-doped TeO2-ZnO-La2O3 modified tellurite glasses were prepared by the conventional melt-quenchi...
Er3+ doped tellurite glasses of molar composition (80-x)TeO2-18ZnO-1MgO-1Li2O-(x)Er2O3 system (0.5mo...
Series of Er3+ doped tellurite glass of the TeO2-PbO-Li2O-Nd2O3-Er2O3 system was successfully been m...