Cold-sprayed Ni-based superalloy coatings offer new possibilities for manufacturing and repairing damaged components, such as gas turbine blades or other parts of aircraft engines. This development shines a new light on the conventional additive manufacturing technologies and significantly broadens application fields of cold spray. The idea is that cold spray can contribute to improving the fatigue properties of manufacturing and repaired components. This study deals with the analysis of the microstructural and mechanical properties of IN625 cold-sprayed coatings on V-notched carbon steel substrate. Process conditions of 1000 degrees C and 50bar were employed to produce coatings in V-notched (60 degrees and 90 degrees) samples in order to e...
Cold-spray coatings were produced by FeCoCrNiMn high-entropy alloy powders deposited on carbon steel...
Cold spray technology is an emerging spray coating process that uses high velocity (kinetic energy) ...
High-temperature corrosion fatigue, a combination of corrosion with a fatigue cycle, is an emerging ...
Cold-sprayed Ni-based superalloy coatings offer new possibilities for manufacturing and repairing da...
NPS NRP Executive SummaryCold dynamic gas spray, better known as cold spray, has generated much inte...
NPS NRP Project PosterCold dynamic gas spray, better known as cold spray, has generated much interes...
Cold spray technique has been major improved in the last decades, for studying new properties for me...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Surface treatments such as shot peening to inhibit fatigue crack initiation are essential processes ...
Wrought magnesium alloys are considered attractive candidates for structural members in automotive a...
Cold-spray coatings were produced by FeCoCrNiMn high-entropy alloy powders deposited on carbon steel...
Cold spray technology is an emerging spray coating process that uses high velocity (kinetic energy) ...
High-temperature corrosion fatigue, a combination of corrosion with a fatigue cycle, is an emerging ...
Cold-sprayed Ni-based superalloy coatings offer new possibilities for manufacturing and repairing da...
NPS NRP Executive SummaryCold dynamic gas spray, better known as cold spray, has generated much inte...
NPS NRP Project PosterCold dynamic gas spray, better known as cold spray, has generated much interes...
Cold spray technique has been major improved in the last decades, for studying new properties for me...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Cold spray technology has recently gained much attention for applications beyond its primary cause o...
Surface treatments such as shot peening to inhibit fatigue crack initiation are essential processes ...
Wrought magnesium alloys are considered attractive candidates for structural members in automotive a...
Cold-spray coatings were produced by FeCoCrNiMn high-entropy alloy powders deposited on carbon steel...
Cold spray technology is an emerging spray coating process that uses high velocity (kinetic energy) ...
High-temperature corrosion fatigue, a combination of corrosion with a fatigue cycle, is an emerging ...