Defects in the crystalline structure of quartz facilitate the connection with the alkali hydroxides, since under a high alkalinity condition (e.g., in concrete), the Si-O bonds of quartz are easily broken. This study set out to investigate the influence of the deformation structures of quartz on its susceptibility to the alkali–silica reaction. A granite, a protomylonite, and a mylonite were selected for this study. Using optical microscopy, the quartz grains contained in these rocks were quantified and their texture characterized. The quartz samples extracted from the rocks were analyzed by magnetic nuclear resonance, to evaluate their potential for dissolving silica as well as changes in their atomic scale before and after the react...
Alkali silica reaction (ASR) is a harmful phenomenon occurring as a result of chemical interactions ...
The “Sierras Pampeanas de Córdoba” (Argentina) is an igneous-metamorphic complex affected by shear z...
The mechanochemical activation (dry grinding) causes destruction in the crystal structure of kaolini...
Defects in the crystalline structure of quartz facilitate the connection with the alkali hydroxides,...
This paper presents research on the influence of quartz deformation in aggregates for the developmen...
It has been known for a long time that strained, microcrystalline or cryptocrystalline quartz-bearin...
This paper presents research on the influence of quartz deformation in aggregates for the developmen...
Granite is the most important source of construction aggregate in Peninsular Malaysia and is widely ...
The present study is a contribution to the understanding of \u3b1-quartz reactivity towards the alka...
The alkali-silica reaction is one of the most damaging chemical reactions taking place in concrete, ...
(AJ) Even today, alkali-silica reaction is a significant problem in concrete-making industry. It was...
Maarten Broekmans has studied the alkali-silica reaction in two Dutch concretes by means of optical ...
Reliable assessment of the potential of quartz in aggregate to develop deleterious alkali-silica rea...
Reliable assessment of the potential alkali reactivity of aggregate to develop deleterious alkali-si...
Les liens qui unissent la structure et les propriétés physiques, chimiques des matériaux sont très i...
Alkali silica reaction (ASR) is a harmful phenomenon occurring as a result of chemical interactions ...
The “Sierras Pampeanas de Córdoba” (Argentina) is an igneous-metamorphic complex affected by shear z...
The mechanochemical activation (dry grinding) causes destruction in the crystal structure of kaolini...
Defects in the crystalline structure of quartz facilitate the connection with the alkali hydroxides,...
This paper presents research on the influence of quartz deformation in aggregates for the developmen...
It has been known for a long time that strained, microcrystalline or cryptocrystalline quartz-bearin...
This paper presents research on the influence of quartz deformation in aggregates for the developmen...
Granite is the most important source of construction aggregate in Peninsular Malaysia and is widely ...
The present study is a contribution to the understanding of \u3b1-quartz reactivity towards the alka...
The alkali-silica reaction is one of the most damaging chemical reactions taking place in concrete, ...
(AJ) Even today, alkali-silica reaction is a significant problem in concrete-making industry. It was...
Maarten Broekmans has studied the alkali-silica reaction in two Dutch concretes by means of optical ...
Reliable assessment of the potential of quartz in aggregate to develop deleterious alkali-silica rea...
Reliable assessment of the potential alkali reactivity of aggregate to develop deleterious alkali-si...
Les liens qui unissent la structure et les propriétés physiques, chimiques des matériaux sont très i...
Alkali silica reaction (ASR) is a harmful phenomenon occurring as a result of chemical interactions ...
The “Sierras Pampeanas de Córdoba” (Argentina) is an igneous-metamorphic complex affected by shear z...
The mechanochemical activation (dry grinding) causes destruction in the crystal structure of kaolini...