Abstract Background The purpose of this study is to evaluate the wear and fracture strength of crowns and three-unit partial fixed dental prosthesis (FDP) fabricated using by Bruxzir and Incoris TZI as recently introduced monolithic zirconia materials. Methods A total of sixteen crowns and sixteen three-unit FDPs were fabricated using Bruxzir and Incoris TZI (n = 8). All specimens were subjected to a 2-body wear test in a dual axis chewing simulator for 1,200,000 loading cycles against steatite antagonist balls. The fracture strength and volumetric loss were recorded. The obtained data were statistically analyzed by 2-way ANOVA testing (α = 0.05). Results The mean volumetric loss of the crowns was higher than that of the three-unit FDPs (p ...
Objective: The purpose of this in-vitro study is to evaluate fracture resistance of two monolithic a...
The aim of this study is to determine the minimum required thickness of a monolithic zirconia crown ...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
Purpose: The aim of this study was to evaluate the effect of wall thickness on load at fracture of m...
This study compared the fracture resistance of monolithic and veneered all-ceramic four-unit posteri...
The aim of the current investigation was to evaluate the fracture resistance of one-piece zirconia ...
Objective. To investigate the fracture resistance and phase composition of tooth supported four-unit...
The aim of the current investigation was to evaluate the fracture resistance of one-piece zirconia ...
AIM: The aim of the present study was to investigate fracture resistance of implant-supported zircon...
Aim: The aim of the present study was to investigate fracture resistance of implant‐supported zirco...
Objective: The purpose of this in-vitro study is to evaluate fracture resistance of two monolithic a...
The aim of this study is to determine the minimum required thickness of a monolithic zirconia crown ...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...
Purpose: The aim of this study was to evaluate the effect of wall thickness on load at fracture of m...
This study compared the fracture resistance of monolithic and veneered all-ceramic four-unit posteri...
The aim of the current investigation was to evaluate the fracture resistance of one-piece zirconia ...
Objective. To investigate the fracture resistance and phase composition of tooth supported four-unit...
The aim of the current investigation was to evaluate the fracture resistance of one-piece zirconia ...
AIM: The aim of the present study was to investigate fracture resistance of implant-supported zircon...
Aim: The aim of the present study was to investigate fracture resistance of implant‐supported zirco...
Objective: The purpose of this in-vitro study is to evaluate fracture resistance of two monolithic a...
The aim of this study is to determine the minimum required thickness of a monolithic zirconia crown ...
The purpose of this study was to evaluate the effect of design and surface finishing on fracture str...