In this work, the relations between the replication quality of random, coarse textured, surfaces with the injection-moulding process has been analysed through 3D areal characterisation techniques. The multi-scale surface approach has been applied to effectively separate the main surface components, roughness, waviness and form. Amplitude, functional, hybrid and spatial parameters, as well as alternative surface characteristics such as the number of micro-cavities (NG), grain area () and grain volume (GV) were used as a way to determine the influence of the manufacturing process on the replication quality of the mould texture, either at the macro- or micro-scale. A model to quantify the effect of the injection-moulding parameters on surface ...
Surface properties of injection molded parts have a strong effect on the visual and haptic perceptio...
Micro-injection moulding is one of the key technologies for micro-manufacture and is widely used as ...
The possibility of tailoring key surface properties through the injection molding process makes it i...
In this work, the relations between the replication quality of random, coarse textured, surfaces wit...
Micro-injection moulding is one of the key technologies for micro-manufacture because of its mass-pr...
The surface quality that results when replicating micro features is one of the most important proces...
Micro-injection moulding is one of the key technologies for micro-manufacture because of its mass-pr...
Injection moulding of micro-featured plastic parts is becoming more and more important for applicati...
The achievement of an adequate accuracy of the microinjection molding process applied to the replica...
Adding textures to surfaces is known to improve the external appearance of injection moulded compone...
Injection moulding is commonly used for the cost effective mass production of plastic parts. Cavity ...
A novel assessment method based on three-dimensions technology has been proposed for analysing the s...
Micro-injection-moulding as a replication method is one of the key technologies for micro-manufactur...
Mass production of micro-structured surfaces has gain great interest for optical and micro fluidic d...
Surface properties of injection molded parts have a strong effect on the visual and haptic perceptio...
Micro-injection moulding is one of the key technologies for micro-manufacture and is widely used as ...
The possibility of tailoring key surface properties through the injection molding process makes it i...
In this work, the relations between the replication quality of random, coarse textured, surfaces wit...
Micro-injection moulding is one of the key technologies for micro-manufacture because of its mass-pr...
The surface quality that results when replicating micro features is one of the most important proces...
Micro-injection moulding is one of the key technologies for micro-manufacture because of its mass-pr...
Injection moulding of micro-featured plastic parts is becoming more and more important for applicati...
The achievement of an adequate accuracy of the microinjection molding process applied to the replica...
Adding textures to surfaces is known to improve the external appearance of injection moulded compone...
Injection moulding is commonly used for the cost effective mass production of plastic parts. Cavity ...
A novel assessment method based on three-dimensions technology has been proposed for analysing the s...
Micro-injection-moulding as a replication method is one of the key technologies for micro-manufactur...
Mass production of micro-structured surfaces has gain great interest for optical and micro fluidic d...
Surface properties of injection molded parts have a strong effect on the visual and haptic perceptio...
Micro-injection moulding is one of the key technologies for micro-manufacture and is widely used as ...
The possibility of tailoring key surface properties through the injection molding process makes it i...