In calcific aortic valve disease (CAVD), microcalcifications originating from nanoscale calcifying vesicles disrupt the aortic valve (AV) leaflets, which consist of three (biomechanically) distinct layers: the fibrosa, spongiosa, and ventricularis. CAVD has no pharmacotherapy and lacks in vitro models as a result of complex valvular biomechanical features surrounding resident mechanosensitive valvular interstitial cells (VICs). We measured layer-specific mechanical properties of the human AV and engineered a three-dimensional (3D)-bioprinted CAVD model that recapitulates leaflet layer biomechanics for the first time. Human AV leaflet layers were separated by microdissection, and nanoindentation determined layer-specific Young’s moduli. Meth...
The fibrosa layer of a cardiac aortic valve is composed mostly of a dense network of type I collagen...
Coordinated movement of cardiac valves controls unidirectional flow of the blood with every heart be...
Calcific aortic valve disease (CAVD) is associated with significant cardiovascular morbidity. While ...
\u3cp\u3eIn calcific aortic valve disease (CAVD), microcalcifications originating from nanoscale cal...
In calcific aortic valve disease (CAVD), microcalcifications originating from nanoscale calcifying v...
In calcific aortic valve disease (CAVD), microcalcifications originating from nanoscale calcifying v...
The main objectives of the research presented in this thesis are to develop a representative in vitr...
PURPOSE: Calcific aortic valve disease (CAVD) is the most prevalent valve disease in the Western wor...
Calcified aortic valve disease (CAVD) is an increasingly prevalent pathology that often manifests in...
Calcific aortic valve disease (CAVD) is one of the most common causes of cardiovascular disease in N...
Aortic valve disease (AVD) is a large contributor to health costs in the United States affecting 2.8...
Because human aortic valve calcification can only be treated by valve replacement, it is a priority ...
Aortic valve interstitial cells (AVICs) are fibrobast-like cells that reside within all layers of th...
Abstract Digitalization of health care practices is substantially manifesting itself as an effective...
Calcific aortic valve disease (CAVD) is the most common valve disease in the Western world. There is...
The fibrosa layer of a cardiac aortic valve is composed mostly of a dense network of type I collagen...
Coordinated movement of cardiac valves controls unidirectional flow of the blood with every heart be...
Calcific aortic valve disease (CAVD) is associated with significant cardiovascular morbidity. While ...
\u3cp\u3eIn calcific aortic valve disease (CAVD), microcalcifications originating from nanoscale cal...
In calcific aortic valve disease (CAVD), microcalcifications originating from nanoscale calcifying v...
In calcific aortic valve disease (CAVD), microcalcifications originating from nanoscale calcifying v...
The main objectives of the research presented in this thesis are to develop a representative in vitr...
PURPOSE: Calcific aortic valve disease (CAVD) is the most prevalent valve disease in the Western wor...
Calcified aortic valve disease (CAVD) is an increasingly prevalent pathology that often manifests in...
Calcific aortic valve disease (CAVD) is one of the most common causes of cardiovascular disease in N...
Aortic valve disease (AVD) is a large contributor to health costs in the United States affecting 2.8...
Because human aortic valve calcification can only be treated by valve replacement, it is a priority ...
Aortic valve interstitial cells (AVICs) are fibrobast-like cells that reside within all layers of th...
Abstract Digitalization of health care practices is substantially manifesting itself as an effective...
Calcific aortic valve disease (CAVD) is the most common valve disease in the Western world. There is...
The fibrosa layer of a cardiac aortic valve is composed mostly of a dense network of type I collagen...
Coordinated movement of cardiac valves controls unidirectional flow of the blood with every heart be...
Calcific aortic valve disease (CAVD) is associated with significant cardiovascular morbidity. While ...