The hot working behavior of neara titanisiin alloy [MI 834 with a duplex starting microstructure was studied using the technique of processing map. The processing map was interpreted in terns of the microstructural processes occurring during deformation, based on the values of dimensionless parameter q which represents the energy dissipation through microstructural processes. An instability criterion (;<0) was also applied to demarcate the flow instability regions in the processing map. Both the parameters (q and Jr were computed using the experimental data generated by carrying out hot compression tests over a range of temperatures (850-1060 degrees C) and strain rates (3 x 10(-4) - 1/s). The deterministic domains observed under the invest...
TiH2-basd powder metallurgy (PM) is one of the effective ways to prepared high temperature titanium ...
Abstract A new biomaterial Ti–14Cr alloy was designed for biomedical applications. The manufacturing...
The isothermal compression tests of titanium alloy Ti–6.5Al–3.5Mo–1.5Zr–0.3Si with the initial Widma...
AbstractThe hot working behavior of near-α titanium alloy IMI 834 with a duplex starting microstruct...
The high temperature deformation behaviour of cast and homogenised near alpha titanium alloy Titan 2...
Hot compression tests on TiHy 600 alloy (equivalent to IMI 834) is performed using Gleeble-3800® the...
The hot workability of Ti–6Al–4V alloy was investigated according to the measured stress–strain data...
The isothermal compression experiment of as-rolled Ti55 alloy was carried out on a Gleeble-3800 ther...
In recent years, processing maps are being used to design hot working schedules for making near-net ...
The hot working behaviour of near-a titanium alloy - TITAN 29A (equivalent to IMI 834) with an acicu...
Using a dynamic materials model, processing and instability maps have been developed for near-alpha ...
This study investigated the hot deformation behavior of Ti-4Al-1Sn-2Zr-5Mo-8V-2.5Cr alloy through is...
Using a dynamic materials model, processing and instability maps have been developed for near-α tita...
IMI 834 is a near alpha titanium alloy, extensively used for gas turbine engine applications such as...
TiHy 600 alloy is a near alpha titanium alloy, widely used for gas turbine engine applications such ...
TiH2-basd powder metallurgy (PM) is one of the effective ways to prepared high temperature titanium ...
Abstract A new biomaterial Ti–14Cr alloy was designed for biomedical applications. The manufacturing...
The isothermal compression tests of titanium alloy Ti–6.5Al–3.5Mo–1.5Zr–0.3Si with the initial Widma...
AbstractThe hot working behavior of near-α titanium alloy IMI 834 with a duplex starting microstruct...
The high temperature deformation behaviour of cast and homogenised near alpha titanium alloy Titan 2...
Hot compression tests on TiHy 600 alloy (equivalent to IMI 834) is performed using Gleeble-3800® the...
The hot workability of Ti–6Al–4V alloy was investigated according to the measured stress–strain data...
The isothermal compression experiment of as-rolled Ti55 alloy was carried out on a Gleeble-3800 ther...
In recent years, processing maps are being used to design hot working schedules for making near-net ...
The hot working behaviour of near-a titanium alloy - TITAN 29A (equivalent to IMI 834) with an acicu...
Using a dynamic materials model, processing and instability maps have been developed for near-alpha ...
This study investigated the hot deformation behavior of Ti-4Al-1Sn-2Zr-5Mo-8V-2.5Cr alloy through is...
Using a dynamic materials model, processing and instability maps have been developed for near-α tita...
IMI 834 is a near alpha titanium alloy, extensively used for gas turbine engine applications such as...
TiHy 600 alloy is a near alpha titanium alloy, widely used for gas turbine engine applications such ...
TiH2-basd powder metallurgy (PM) is one of the effective ways to prepared high temperature titanium ...
Abstract A new biomaterial Ti–14Cr alloy was designed for biomedical applications. The manufacturing...
The isothermal compression tests of titanium alloy Ti–6.5Al–3.5Mo–1.5Zr–0.3Si with the initial Widma...