The sintering of hardmetal in the solid state is studied. The influence of the WC particle size on the sintering kinetics, the role of the binder phase in the densification process and how sintering depends on the heating conditions are investigated. It is observed that alloys with different WC particle size show quite different structural evolution during sintering, although the densification mechanisms are the same. This is explained by the formation of agglomerates of WC and Co. Hardmetal alloys can sinter very rapidly when high heating rates are used, since rapid heating accelerates the binder spreading and the formation of WC-Co agglomerates. The binder phase (Co) spreads on the WC particles initially as a thin layer. Subsequently, mor...
Most important processes during heat treatment of powder mixtures for production of cermets and hard...
Hardmetals are conventionally manufactured by liquid phase sintering above 1350 °C. Due to their hig...
Cold compaction (200-1900 MPa) and sintering (1250 degrees-1350 degrees C) of cermets based on WC-Co...
The outgassing and sintering processes occurring during the heating period are very decisive for the...
International audienceThe densification of WC-10Co (wt %) alloys is studied in relation with interfa...
This paper evaluated the effect of high-energy milling and sintering temperature on the structural c...
International audienceCemented carbides are used in the cutting tools industry thanks to their excep...
WC-Co hardmetals using different starting powders were densified by spark plasma sintering (SPS). Si...
During the sintering of WC-Co powder compacts reactions occur which determine the properties of the ...
The paper describes the method for producing WC-10wt%Co hard alloy with 99.6% of the theoretical den...
Grain growth and abnormal grain growth in tungsten carbide cobalt composites (cemented carbides, har...
Hard metals are powder metallurgical products composed of WC and Co. Applications for such materials...
The diffusion behaviour of the grain-growth inhibitors (GGI) Cr and V during early sintering stages ...
A new 0.4 mu m WC powder with hardmetal properties based on optimized structures and doping additive...
This work demonstrates an accurate model for solidification of WC-Co powder in thermal spray deposit...
Most important processes during heat treatment of powder mixtures for production of cermets and hard...
Hardmetals are conventionally manufactured by liquid phase sintering above 1350 °C. Due to their hig...
Cold compaction (200-1900 MPa) and sintering (1250 degrees-1350 degrees C) of cermets based on WC-Co...
The outgassing and sintering processes occurring during the heating period are very decisive for the...
International audienceThe densification of WC-10Co (wt %) alloys is studied in relation with interfa...
This paper evaluated the effect of high-energy milling and sintering temperature on the structural c...
International audienceCemented carbides are used in the cutting tools industry thanks to their excep...
WC-Co hardmetals using different starting powders were densified by spark plasma sintering (SPS). Si...
During the sintering of WC-Co powder compacts reactions occur which determine the properties of the ...
The paper describes the method for producing WC-10wt%Co hard alloy with 99.6% of the theoretical den...
Grain growth and abnormal grain growth in tungsten carbide cobalt composites (cemented carbides, har...
Hard metals are powder metallurgical products composed of WC and Co. Applications for such materials...
The diffusion behaviour of the grain-growth inhibitors (GGI) Cr and V during early sintering stages ...
A new 0.4 mu m WC powder with hardmetal properties based on optimized structures and doping additive...
This work demonstrates an accurate model for solidification of WC-Co powder in thermal spray deposit...
Most important processes during heat treatment of powder mixtures for production of cermets and hard...
Hardmetals are conventionally manufactured by liquid phase sintering above 1350 °C. Due to their hig...
Cold compaction (200-1900 MPa) and sintering (1250 degrees-1350 degrees C) of cermets based on WC-Co...