\ua9 2016 Elsevier Ltd. In this paper, the high temperature cyclic and relaxation behaviour of Ni-based superalloy Haynes 282 is investigated. Low-cycle fatigue (LCF) tests with and without hold time have been performed at two elevated temperatures, 650 and 730 \ub0C. The test results are presented and analysed with respect to the cyclic behaviour and the stress relaxation behaviour. Based on this analysis, a Chaboche type of elasto-viscoplastic material model is formulated and calibrated with respect to the cyclic experimental data. Furthermore, the effect of the scatter, observed in the initial yield stresses of the LCF tests, is considered in the calibration of the material model. Finally, a Golos-Ellyin strain energy density fatigue cri...
We present the low-cycle fatigue behavior of a new nickel-based superalloy in the temperature range ...
The low-cycle fatigue (LCF) behavior of a wrought cobalt-base superalloy, Haynes 188, has been inves...
This thesis describes innovative methods used to predict high-stress amplitude, low cycle fatigue (L...
© 2016 Elsevier Ltd. In this paper, the high temperature cyclic and relaxation behaviour of Ni-based...
In this contribution the mechanical behaviour of the Ni-based superalloy Haynes 282, developed for h...
In the aviation industry today there is a trend of increasing operating temperatures in turbine engi...
In gas turbine engines for aerospace propulsion, the assessment of the fatigue damage mechanisms due...
Critical jet engine components are exposed to high temperatures. These components are also required ...
In gas turbine engines for aerospace propulsion, the assessment of the fatigue damage mechanisms due...
In gas turbine engines for aerospace propulsion, the assessment of the fatigue damage mechanisms due...
In gas turbine engines for aerospace propulsion, the assessment of the fatigue damage mechanisms due...
<p>Critical jet engine components are exposed to high temperatures. These components are also requir...
The paper describes the results of fatigue behavior study on cast polycrystalline nickel based supe...
AbstractLow cycle fatigue (LCF) and fatigue-creep tests were conducted under different dwell conditi...
In this paper, total strain-controlled high temperature (760 °C) low cycle fatigue (HTLCF) behaviour...
We present the low-cycle fatigue behavior of a new nickel-based superalloy in the temperature range ...
The low-cycle fatigue (LCF) behavior of a wrought cobalt-base superalloy, Haynes 188, has been inves...
This thesis describes innovative methods used to predict high-stress amplitude, low cycle fatigue (L...
© 2016 Elsevier Ltd. In this paper, the high temperature cyclic and relaxation behaviour of Ni-based...
In this contribution the mechanical behaviour of the Ni-based superalloy Haynes 282, developed for h...
In the aviation industry today there is a trend of increasing operating temperatures in turbine engi...
In gas turbine engines for aerospace propulsion, the assessment of the fatigue damage mechanisms due...
Critical jet engine components are exposed to high temperatures. These components are also required ...
In gas turbine engines for aerospace propulsion, the assessment of the fatigue damage mechanisms due...
In gas turbine engines for aerospace propulsion, the assessment of the fatigue damage mechanisms due...
In gas turbine engines for aerospace propulsion, the assessment of the fatigue damage mechanisms due...
<p>Critical jet engine components are exposed to high temperatures. These components are also requir...
The paper describes the results of fatigue behavior study on cast polycrystalline nickel based supe...
AbstractLow cycle fatigue (LCF) and fatigue-creep tests were conducted under different dwell conditi...
In this paper, total strain-controlled high temperature (760 °C) low cycle fatigue (HTLCF) behaviour...
We present the low-cycle fatigue behavior of a new nickel-based superalloy in the temperature range ...
The low-cycle fatigue (LCF) behavior of a wrought cobalt-base superalloy, Haynes 188, has been inves...
This thesis describes innovative methods used to predict high-stress amplitude, low cycle fatigue (L...