In this work, we report the enhanced catalytic reduction of 4-nitrophenol driven by Fe3O4-Au magnetic nanocomposite interface engineering. A facile solvothermal method is employed for Fe3O4 hollow microspheres and Fe3O4-Au magnetic nanocomposite synthesis via a seed deposition process. Complementary structural, chemical composition and valence state studies validate that the as-obtained samples are formed in a pure magnetite phase. A series of characterizations including conventional scanning/transmission electron microscopy (SEM/TEM), Mössbauer spectroscopy, magnetic testing and elemental mapping is conducted to unveil the structural and physical characteristics of the developed Fe3O4-Au magnetic nanocomposites. By adjusting the quant...
We demonstrated a simple approach for fabricating Au–Fe3O4/PDA hollow nanoparticles as high-performa...
Gold nanoparticles (Au NPs) have been widely employed in catalysis. Here, we report on the synthesis...
Fe3O4 spheres with an average size of 273 nm were prepared in the presence of CTAB by a solvothermal...
In this work, we report the enhanced catalytic reduction of 4-nitrophenol driven by Fe3O4-Au magneti...
In this work, Fe3O4 magnetic nanoparticles (MNPs) were produced using the co-precipitation method. T...
In this paper, a facile route has been developed to prepare magnetic trimetallic Au-Ag-γ-Fe2O3/...
Magnetic supports were prepared by coating Fe3O4 nanoparticles with polystyrene (PS). The target nan...
An environmentally benign magnetic gold nanoparticles (AuNPs) catalyst supported onto thioctic acid ...
In this research, a facile and effective approach was developed for the preparation of well-designed...
Abstract A new and efficient catalyst has been designed and prepared via in situ immobilization of A...
Highly stable gold nanoparticles immobilized on the surface of amine-functionalized nanocomposite mi...
Magnetically recyclable nanocatalysts with excellent performance are urgent need in heterogeneous ca...
A novel Fe3O4@Au nanocatalyst was successfully self-assembled induced by host-guest interaction betw...
In recent days, the green synthesized nanomagnetic biocomposites have been evolved with tremendous p...
This work reports a novel Fe<sub>3</sub>O<sub>4</sub>@polydopamine/Au/polydopamine core/shell nanoco...
We demonstrated a simple approach for fabricating Au–Fe3O4/PDA hollow nanoparticles as high-performa...
Gold nanoparticles (Au NPs) have been widely employed in catalysis. Here, we report on the synthesis...
Fe3O4 spheres with an average size of 273 nm were prepared in the presence of CTAB by a solvothermal...
In this work, we report the enhanced catalytic reduction of 4-nitrophenol driven by Fe3O4-Au magneti...
In this work, Fe3O4 magnetic nanoparticles (MNPs) were produced using the co-precipitation method. T...
In this paper, a facile route has been developed to prepare magnetic trimetallic Au-Ag-γ-Fe2O3/...
Magnetic supports were prepared by coating Fe3O4 nanoparticles with polystyrene (PS). The target nan...
An environmentally benign magnetic gold nanoparticles (AuNPs) catalyst supported onto thioctic acid ...
In this research, a facile and effective approach was developed for the preparation of well-designed...
Abstract A new and efficient catalyst has been designed and prepared via in situ immobilization of A...
Highly stable gold nanoparticles immobilized on the surface of amine-functionalized nanocomposite mi...
Magnetically recyclable nanocatalysts with excellent performance are urgent need in heterogeneous ca...
A novel Fe3O4@Au nanocatalyst was successfully self-assembled induced by host-guest interaction betw...
In recent days, the green synthesized nanomagnetic biocomposites have been evolved with tremendous p...
This work reports a novel Fe<sub>3</sub>O<sub>4</sub>@polydopamine/Au/polydopamine core/shell nanoco...
We demonstrated a simple approach for fabricating Au–Fe3O4/PDA hollow nanoparticles as high-performa...
Gold nanoparticles (Au NPs) have been widely employed in catalysis. Here, we report on the synthesis...
Fe3O4 spheres with an average size of 273 nm were prepared in the presence of CTAB by a solvothermal...