This study presents the results of a detailed investigation of metastability and susceptibility to deformation induced α’-martensite formation of several austenitic steels (AISI 304, AISI 321, AISI 348 and two batches from AISI 347) in the solution-annealed state. Besides conventional characterization of metastability by calculating stacking-fault energy and threshold temperature (designated as MS and Md30), the present work introduced a new method for determining susceptibility to α’-martensite formation. The method was based on dynamically applied local plastic deformation and non-destructive micro-magnetic measurement of α’-martensite content. The parameter Iξ was established, which correlated very well with the grade of α’-martensite fo...
AbstractSurface treatment, e.g. shot peening and deep rolling, is popular in aero engine industry, w...
AbstractThe effect of deformation induced martensite on the HCF and VHCF properties of austenitic st...
Total strain-controlled low-cycle fatigue tests were performed at room temperature on a high alloyed...
This study presents the results of a detailed investigation of metastability and susceptibility to d...
This study presents the results of a detailed investigation of metastability and susceptibility to d...
AbstractFatigue behavior and phase transformation in the metastable austenitic steels AISI 304, 321 ...
The effect of applied total strain range on the critical condition necessary for the onset of α'-mar...
The effect of applied total strain range on the critical condition necessary for the onset of α'-mar...
AbstractFatigue behavior and phase transformation in the metastable austenitic steels AISI 304, 321 ...
The plastic deformation accumulated during fatigue testing can induce the transformation of austeni...
The plastic deformation accumulated during fatigue testing can induce the transformation of austenit...
The plastic deformation accumulated during fatigue testing can induce the transformation of austenit...
According to their excellent mechanical and technological properties, i.e. high toughness, as well a...
Total strain-controlled low-cycle fatigue tests were performed at room temperature on a high alloyed...
Metastable austenitic stainless steels are currently used in applications where severe forming opera...
AbstractSurface treatment, e.g. shot peening and deep rolling, is popular in aero engine industry, w...
AbstractThe effect of deformation induced martensite on the HCF and VHCF properties of austenitic st...
Total strain-controlled low-cycle fatigue tests were performed at room temperature on a high alloyed...
This study presents the results of a detailed investigation of metastability and susceptibility to d...
This study presents the results of a detailed investigation of metastability and susceptibility to d...
AbstractFatigue behavior and phase transformation in the metastable austenitic steels AISI 304, 321 ...
The effect of applied total strain range on the critical condition necessary for the onset of α'-mar...
The effect of applied total strain range on the critical condition necessary for the onset of α'-mar...
AbstractFatigue behavior and phase transformation in the metastable austenitic steels AISI 304, 321 ...
The plastic deformation accumulated during fatigue testing can induce the transformation of austeni...
The plastic deformation accumulated during fatigue testing can induce the transformation of austenit...
The plastic deformation accumulated during fatigue testing can induce the transformation of austenit...
According to their excellent mechanical and technological properties, i.e. high toughness, as well a...
Total strain-controlled low-cycle fatigue tests were performed at room temperature on a high alloyed...
Metastable austenitic stainless steels are currently used in applications where severe forming opera...
AbstractSurface treatment, e.g. shot peening and deep rolling, is popular in aero engine industry, w...
AbstractThe effect of deformation induced martensite on the HCF and VHCF properties of austenitic st...
Total strain-controlled low-cycle fatigue tests were performed at room temperature on a high alloyed...