对定向凝固Ni3Al基超合金IC6,以不同功率密度的强脉冲离子束进行辐照,利用X射线衍射分析,研究了辐照后材料表面所产生的物相变化。结果表明:当以低功率密度辐照时,材料表面形成形变织构;随着功率密度的增加,材料表面还会发生部分非晶化;当功率密度进一步增加时,材料表面出现了新相。The phase evolution of the directionally solidified Ni3Al based superalloy IC6 after exposure to intense pulsed ion beams (IPIB) has been studied by X-ray diffraction analysis. It shows that the deformation texture is formed, on the surface layer of the target under IPIB irradiation with a low power density. The minor amorphous gamma' phase can be produced when the target is irradiated by IPIB with a moderate power density. With further increasing the power density of IPIB, a new phase, appears on the irradiated deformation mechanisms.http://gateway.webofknowledge.com/gateway/Gateway.cgi?GWVersion=2...
In this paper it was shown that pulsed electron irradiation forms in the surface layer of the Ni[3]A...
The phenomenon of irradiation softening has recently been noticed for nickel-based single crystal su...
Irradiation Induced Phase Transformation in NiTi Shape Memory Alloy Mr. Thomas Lagrange1; Dr....
The effects of intense pulsed ion beams (IPIB) irradiation (ions of C+ and H+, accelerating voltage ...
The effects of intense pulsed ion beams (IPIB) irradiation (ions of C+ and H+, accelerating voltage ...
Ni3Al base alloy was irradiated by intense pulsed ion beam (IPIB) with 250 kV acceleration voltage, ...
The effects of intense pulsed ion beams (IPIB) irradiation with three kinds of power densities on th...
Intense pulsed ion beams (IPIB) with three different power densities (25, 37.5 and 50 MW/cm2) are em...
An ion beam treatment of high purity single crystal silicon specimens was performed with different s...
研究了强脉冲离子束(IPIB)对Ni/Ti和Al/Ti体系的混合效果,并与常规离子束混合进行了对比研究,表明 IPIB 辐照确实获得了比常规离子束辐照更厚的混合层,且混合效率远高于常规离子束.但对于不...
以Fourier瞬态传热方程为基础,确定了强流脉冲离子束(HIPIB)热效应的基本传热方程,对靶材45钢进行不同能量参数的HIPIB辐照热效应的模拟计算.针对离子注入金属内部的情况,在模拟束流加载方式...
It was found that some craters appeared on the irradiated surfaces that have been melted under inten...
强脉冲离子束作为一种闪光热源在材料表面改性方面具有广泛的应用.烧蚀效应对于强脉冲离子束与物质相互作用以及强脉冲离子束薄膜沉积过程具有重要的影响.因此,分析强脉冲离子束的烧蚀过程和机理对于优化其应用具有...
Multilayers of Ni-2lAl and Ni-ZOCr-1OAl were subjected to ion beam mixing using 350 keV Ni+ ions and...
在回顾和总结强脉冲电子束表面改性实验的基础上,利用有限元数值计算方法对强脉冲电子束辐照铝和304不锈钢产生的温度场进行模拟,给出了靶的近表面区域流体状态存在的特征尺度和特征时间,并对不同材料特性下熔坑...
In this paper it was shown that pulsed electron irradiation forms in the surface layer of the Ni[3]A...
The phenomenon of irradiation softening has recently been noticed for nickel-based single crystal su...
Irradiation Induced Phase Transformation in NiTi Shape Memory Alloy Mr. Thomas Lagrange1; Dr....
The effects of intense pulsed ion beams (IPIB) irradiation (ions of C+ and H+, accelerating voltage ...
The effects of intense pulsed ion beams (IPIB) irradiation (ions of C+ and H+, accelerating voltage ...
Ni3Al base alloy was irradiated by intense pulsed ion beam (IPIB) with 250 kV acceleration voltage, ...
The effects of intense pulsed ion beams (IPIB) irradiation with three kinds of power densities on th...
Intense pulsed ion beams (IPIB) with three different power densities (25, 37.5 and 50 MW/cm2) are em...
An ion beam treatment of high purity single crystal silicon specimens was performed with different s...
研究了强脉冲离子束(IPIB)对Ni/Ti和Al/Ti体系的混合效果,并与常规离子束混合进行了对比研究,表明 IPIB 辐照确实获得了比常规离子束辐照更厚的混合层,且混合效率远高于常规离子束.但对于不...
以Fourier瞬态传热方程为基础,确定了强流脉冲离子束(HIPIB)热效应的基本传热方程,对靶材45钢进行不同能量参数的HIPIB辐照热效应的模拟计算.针对离子注入金属内部的情况,在模拟束流加载方式...
It was found that some craters appeared on the irradiated surfaces that have been melted under inten...
强脉冲离子束作为一种闪光热源在材料表面改性方面具有广泛的应用.烧蚀效应对于强脉冲离子束与物质相互作用以及强脉冲离子束薄膜沉积过程具有重要的影响.因此,分析强脉冲离子束的烧蚀过程和机理对于优化其应用具有...
Multilayers of Ni-2lAl and Ni-ZOCr-1OAl were subjected to ion beam mixing using 350 keV Ni+ ions and...
在回顾和总结强脉冲电子束表面改性实验的基础上,利用有限元数值计算方法对强脉冲电子束辐照铝和304不锈钢产生的温度场进行模拟,给出了靶的近表面区域流体状态存在的特征尺度和特征时间,并对不同材料特性下熔坑...
In this paper it was shown that pulsed electron irradiation forms in the surface layer of the Ni[3]A...
The phenomenon of irradiation softening has recently been noticed for nickel-based single crystal su...
Irradiation Induced Phase Transformation in NiTi Shape Memory Alloy Mr. Thomas Lagrange1; Dr....