Atomic force microscopy (AFM) combined with nanoindentation technique was used to definitely, site-specifically, test the nanomechanical properties, including nanohardness and elastic modulus, of the isolated domains within single enamel, the prisms and the surrounding sheaths, of mature human maxillary third molars. In this way, it is for the first time that evident differences of nanomechanical properties were revealed between these domains. The nanohardness and elastic modulus of the sheaths were about 73.6% and 52.7% lower than those of the prisms, respectively. Measuring the residual impressions with AFM supported the similar conclusion. The variations of mechanical properties in these domains are considered to be mainly relative to th...
This study examines the properties of nanobased dental restorative materials with nanoindentation me...
Surface topography, microstructure, and micromechanical properties of human lamellar bone were chara...
In the present work, nanoindentation technique has been utilised to study the physics of deformation...
Nanohardness and elastic modulus of enamel and dentin were measured by nanoindentation method with V...
Nanoindentation is a relatively new technique used to gain an understanding of the mechanical proper...
In this paper, the usefulness of the specimen shaping ability of focused ion beam (FIB) milling in t...
Objective. Tooth enamel has unsurpassed hardness and stiffness among mammalian tissue structures. Su...
Nanoindentation has recently emerged to be the primary method to study the mechanical behavior and r...
The recently developed nanoindentation technique was used to measure hardness and Young's modulus of...
Introduction: Although it is apparent that teeth become more susceptible to fracture after root cana...
Abstract This study aims to investigate the gradient nanomechanical behavior of dental fluorosis ena...
Objectives/Methods: From a materials scientist's perspective, dental materials used for tooth r...
Developmental defects in dental enamel pose significant clinical challenges which have highlighted o...
Objectives/Methods: From a materials scientist's perspective, dental materials used for tooth repair...
The analysis of mechanical properties on a nanometer scale is a useful tool for combining informatio...
This study examines the properties of nanobased dental restorative materials with nanoindentation me...
Surface topography, microstructure, and micromechanical properties of human lamellar bone were chara...
In the present work, nanoindentation technique has been utilised to study the physics of deformation...
Nanohardness and elastic modulus of enamel and dentin were measured by nanoindentation method with V...
Nanoindentation is a relatively new technique used to gain an understanding of the mechanical proper...
In this paper, the usefulness of the specimen shaping ability of focused ion beam (FIB) milling in t...
Objective. Tooth enamel has unsurpassed hardness and stiffness among mammalian tissue structures. Su...
Nanoindentation has recently emerged to be the primary method to study the mechanical behavior and r...
The recently developed nanoindentation technique was used to measure hardness and Young's modulus of...
Introduction: Although it is apparent that teeth become more susceptible to fracture after root cana...
Abstract This study aims to investigate the gradient nanomechanical behavior of dental fluorosis ena...
Objectives/Methods: From a materials scientist's perspective, dental materials used for tooth r...
Developmental defects in dental enamel pose significant clinical challenges which have highlighted o...
Objectives/Methods: From a materials scientist's perspective, dental materials used for tooth repair...
The analysis of mechanical properties on a nanometer scale is a useful tool for combining informatio...
This study examines the properties of nanobased dental restorative materials with nanoindentation me...
Surface topography, microstructure, and micromechanical properties of human lamellar bone were chara...
In the present work, nanoindentation technique has been utilised to study the physics of deformation...