A model of reactive hot pressing of zirconium carbide (ZrCx, 0.5 , x , 1) has been constructed that incorporates four processes that occur in parallel: creep of zirconium (Zr), reaction of Zr and carbon (C), increase in volume fraction of hard phase with progressive reaction that reduces the creep of Zr and, finally, de-densification associated with volume reduction during reaction. The reasonable agreement of the model with experimental results verifies that plastic deformation of Zr is the main factor that is responsible for the low-temperature reactive densification of ZrC and that ZrC may be treated as a rigid inclusion that contributes little to densification. It predicts that densification is impaired by increasing carbon stoichiometr...
Zirconium carbide ceramics were prepared by carbothermal reduction of ZrO2 and C that were mixed by ...
Dense ZrB2–SiC (25–30 vol%) composites have been produced by reactive hot pressing using stoichiomet...
ZrB2 was mixed with 0.5 wt% carbon and up to 10 vol% ZrC and densified by hot-pressing at 2000 °C. A...
A model of reactive hot pressing of zirconium carbide (ZrCx, 0.5 , x , 1) has been constructed that ...
A model of reactive hot pressing of zirconium carbide (ZrCx, 0.5 < x < 1) has been constructed that ...
Densification mechanisms involved during reactive hot pressing (RHP) of zirconium carbide (ZrC) have...
The effect of applied pressure on reactive hot pressing (RHP) of zirconium (Zr):graphite (C) in mola...
International audienceThe hot-pressing kinetics of zirconium carbide were studied between 1700 and 2...
Reactive hot pressing (RHP) as a low temperature processing route is explored in the present work. F...
Synthesis and densification of monolithic zirconium carbide (ZrC) has been carried out by reactive h...
Synthesis and densification of monolithic zirconium carbide (ZrC) has been carried out by reactive h...
ZrB2‐ZrCx composites were produced using Zr:B4C powder mixtures in the molar ratios of 3:1, 3.5:1, 4...
Spark plasma sintering (SPS) has been employed to consolidate a micron-sized zirconium carbide (ZrC)...
Dense ZrB2-ZrC and ZrB2-ZrC x∼0.67 composites have been produced by reactive hot pressing (RHP) of ...
The dominant densification mechanisms for hot pressing of ZrB2-20 vol.% SiC composite at different h...
Zirconium carbide ceramics were prepared by carbothermal reduction of ZrO2 and C that were mixed by ...
Dense ZrB2–SiC (25–30 vol%) composites have been produced by reactive hot pressing using stoichiomet...
ZrB2 was mixed with 0.5 wt% carbon and up to 10 vol% ZrC and densified by hot-pressing at 2000 °C. A...
A model of reactive hot pressing of zirconium carbide (ZrCx, 0.5 , x , 1) has been constructed that ...
A model of reactive hot pressing of zirconium carbide (ZrCx, 0.5 < x < 1) has been constructed that ...
Densification mechanisms involved during reactive hot pressing (RHP) of zirconium carbide (ZrC) have...
The effect of applied pressure on reactive hot pressing (RHP) of zirconium (Zr):graphite (C) in mola...
International audienceThe hot-pressing kinetics of zirconium carbide were studied between 1700 and 2...
Reactive hot pressing (RHP) as a low temperature processing route is explored in the present work. F...
Synthesis and densification of monolithic zirconium carbide (ZrC) has been carried out by reactive h...
Synthesis and densification of monolithic zirconium carbide (ZrC) has been carried out by reactive h...
ZrB2‐ZrCx composites were produced using Zr:B4C powder mixtures in the molar ratios of 3:1, 3.5:1, 4...
Spark plasma sintering (SPS) has been employed to consolidate a micron-sized zirconium carbide (ZrC)...
Dense ZrB2-ZrC and ZrB2-ZrC x∼0.67 composites have been produced by reactive hot pressing (RHP) of ...
The dominant densification mechanisms for hot pressing of ZrB2-20 vol.% SiC composite at different h...
Zirconium carbide ceramics were prepared by carbothermal reduction of ZrO2 and C that were mixed by ...
Dense ZrB2–SiC (25–30 vol%) composites have been produced by reactive hot pressing using stoichiomet...
ZrB2 was mixed with 0.5 wt% carbon and up to 10 vol% ZrC and densified by hot-pressing at 2000 °C. A...