Uniform and well-dispersed quasi-spherical YVO4:Ln(3+) (Ln Eu, Dy) nanoparticles have been successfully synthesized through a solvothermal approach using EG and PVP as solvent and surfactant, respectively. SEM and TEM images indicate that the as-obtained quasispheres are composed of tiny packed nanocrystallites. The YVO4:Eu3+ and YVO4:Dy3+ samples show strong red and yellow light emissions under ultraviolet excitation. The luminescence intensities of the phosphors are greatly enhanced by co-doping Ba2+ ions into the YVO4 host lattice. Nitrogen adsorption-desorption measurements reveals that the as-synthesized luminescent quasi-spherical nanoparticles have a porous structure, which might find potential applications in the fields of luminesce...
Colloidal, organic solvent-soluble Ln3+-doped LaVO4 nanoparticles have been synthesized by a precipi...
Monodisperse YVO4:Eu3+ submicrocrystals with uniform morphologies have been successfully synthesized...
YVO4 nanocrystals doped with 10.0 mol% Eu3+ have been synthesized from an aqueous solution of ( Y, E...
Well-dispersed YVO4:Ln(3+) (Ln = Eu, Dy, and Sm) nanocrystals with uniform morphology and size have ...
Rare-earth ions (Eu3+, Dy3+, Sm3+) doped YVO4 microspheres with uniform morphologies were successful...
Large-scale spindle-like YVO4 particles with an euatorial diameter of 100-150 nm and a length of 300...
In this paper nanosized luminescent materials YVO4:Sm and YVO4:Dy were synthesized by complex-based ...
YVO4 nano/microcrystals with multiform morphologies, such as nanoparticles, microdoughnut, micropanc...
A simple and single-step method for the production of Ln-doped YVO 4 nanocrystals and their simultan...
Nano-sized particles of monoclinic-LaVO4 were prepared in a short reaction time of 30 minutes by emp...
Nano-sized particles of monoclinic-LaVO4 were prepared in a short reaction time of 30 minutes by emp...
Nano-sized particles of monoclinic-LaVO4 were prepared in a short reaction time of 30 minutes by emp...
Nano-sized particles of monoclinic-LaVO4 were prepared in a short reaction time of 30 minutes by emp...
In the past, an Eu3+-doped YVO4 bulk phosphor with a photoluminescence quantum yield (PLQY) of 70% w...
Nano-sized particles of monoclinic-LaVO4 were prepared in a short reaction time of 30 minutes by emp...
Colloidal, organic solvent-soluble Ln3+-doped LaVO4 nanoparticles have been synthesized by a precipi...
Monodisperse YVO4:Eu3+ submicrocrystals with uniform morphologies have been successfully synthesized...
YVO4 nanocrystals doped with 10.0 mol% Eu3+ have been synthesized from an aqueous solution of ( Y, E...
Well-dispersed YVO4:Ln(3+) (Ln = Eu, Dy, and Sm) nanocrystals with uniform morphology and size have ...
Rare-earth ions (Eu3+, Dy3+, Sm3+) doped YVO4 microspheres with uniform morphologies were successful...
Large-scale spindle-like YVO4 particles with an euatorial diameter of 100-150 nm and a length of 300...
In this paper nanosized luminescent materials YVO4:Sm and YVO4:Dy were synthesized by complex-based ...
YVO4 nano/microcrystals with multiform morphologies, such as nanoparticles, microdoughnut, micropanc...
A simple and single-step method for the production of Ln-doped YVO 4 nanocrystals and their simultan...
Nano-sized particles of monoclinic-LaVO4 were prepared in a short reaction time of 30 minutes by emp...
Nano-sized particles of monoclinic-LaVO4 were prepared in a short reaction time of 30 minutes by emp...
Nano-sized particles of monoclinic-LaVO4 were prepared in a short reaction time of 30 minutes by emp...
Nano-sized particles of monoclinic-LaVO4 were prepared in a short reaction time of 30 minutes by emp...
In the past, an Eu3+-doped YVO4 bulk phosphor with a photoluminescence quantum yield (PLQY) of 70% w...
Nano-sized particles of monoclinic-LaVO4 were prepared in a short reaction time of 30 minutes by emp...
Colloidal, organic solvent-soluble Ln3+-doped LaVO4 nanoparticles have been synthesized by a precipi...
Monodisperse YVO4:Eu3+ submicrocrystals with uniform morphologies have been successfully synthesized...
YVO4 nanocrystals doped with 10.0 mol% Eu3+ have been synthesized from an aqueous solution of ( Y, E...