We report the synthesis of ceria/polymer hybrid nanoparticles and their use as effective supported catalysts for the hydration of nitriles to amide, exemplified with the conversion of 2-cyanopiridine to 2-picolinamide. The polymeric cores, made of either polystyrene (PS) or poly(methyl methacrylate) (PMMA), are prepared by miniemulsion copolymerization in the presence of different functional comonomers that provide carboxylic or phosphate groups: acrylic acid, maleic acid, and ethylene glycol methacrylate phosphate. The functional groups of the comonomers generate a corona around the main polymer particle and serve as nucleating agents for the in situ crystallization of cerium(IV) oxide. The obtained hybrid nanoparticles can be easily red...
Ceria nanoparticles (average particle size: 8nm) have been obtained by the calcination of alginate a...
The most distinguished advantage to use colloidal methods for catalyst preparation is that the size ...
Ceria nanopowders were prepared by varying surfactant (2.5%, 5% and 10% PEG) and solution concentrat...
The three-component condensation of aldehydes, β-ketoesters and urea has been carried out in water u...
The catalytic performance of small Pd-nanoparticles (NPs) (2.0 nm), partially covered by chemisorbed...
A simple, one-step synthesis of 4-vinylpyridine polymer crosslinked with 2% divinylbenzene [poly(4vp...
The dehydration of aldoximes into nitriles has been performed in the presence of various metal oxide...
A monodisperse Pt/ceria hybrid with controlled nanoporous structure was fabricated with the aid of p...
Ceria nanocrystals with a cube shape were synthesized from the hydrolytic sol-gel reaction of cerium...
Mesoporous cerium oxide (CeO2) nanoparticles act as an effective heterogeneous catalyst for the tran...
Polymethylmethacrylate (PMMA)/ceria composite fibres were synthesized by using a sequential combinat...
Polymethylmethacrylate (PMMA)/ceria composite fibres were synthesized by using a sequential combinat...
Zirconium doped ceria nanoparticles are found to be efficient heterogeneous catalysts for the multic...
To test the potential of heterogeneous catalysts for the nylon-6 synthesis from 6-aminocapronitrile,...
To test the potential of heterogeneous catalysts for the nylon-6 synthesis from 6-aminocapronitrile,...
Ceria nanoparticles (average particle size: 8nm) have been obtained by the calcination of alginate a...
The most distinguished advantage to use colloidal methods for catalyst preparation is that the size ...
Ceria nanopowders were prepared by varying surfactant (2.5%, 5% and 10% PEG) and solution concentrat...
The three-component condensation of aldehydes, β-ketoesters and urea has been carried out in water u...
The catalytic performance of small Pd-nanoparticles (NPs) (2.0 nm), partially covered by chemisorbed...
A simple, one-step synthesis of 4-vinylpyridine polymer crosslinked with 2% divinylbenzene [poly(4vp...
The dehydration of aldoximes into nitriles has been performed in the presence of various metal oxide...
A monodisperse Pt/ceria hybrid with controlled nanoporous structure was fabricated with the aid of p...
Ceria nanocrystals with a cube shape were synthesized from the hydrolytic sol-gel reaction of cerium...
Mesoporous cerium oxide (CeO2) nanoparticles act as an effective heterogeneous catalyst for the tran...
Polymethylmethacrylate (PMMA)/ceria composite fibres were synthesized by using a sequential combinat...
Polymethylmethacrylate (PMMA)/ceria composite fibres were synthesized by using a sequential combinat...
Zirconium doped ceria nanoparticles are found to be efficient heterogeneous catalysts for the multic...
To test the potential of heterogeneous catalysts for the nylon-6 synthesis from 6-aminocapronitrile,...
To test the potential of heterogeneous catalysts for the nylon-6 synthesis from 6-aminocapronitrile,...
Ceria nanoparticles (average particle size: 8nm) have been obtained by the calcination of alginate a...
The most distinguished advantage to use colloidal methods for catalyst preparation is that the size ...
Ceria nanopowders were prepared by varying surfactant (2.5%, 5% and 10% PEG) and solution concentrat...