The influence of geometric factors on the galvanic current density distribution for AZ91D coupled to steel was investigated using experimental measurements and a BEM model. The geometric factors were area ratio of anode/cathode, insulation distance between anode and cathode, depth of solution film covering the galvanic couple and the manner of interaction caused by two independent interacting galvanic couples. The galvanic current density distribution calculated from the BEM model was in good agreement with the experimental measurements. The galvanic current density distribution caused by the interaction of two independent galvanic couples can be reasonably predicted as the linear addition of the galvanic current density caused by each indi...
Galvanic corrosion on samples of AZ91D magnesium alloy coupled with 2A12 aluminum alloy during neutr...
The objective of this research was to develop a method for a-priori quantitative prediction of elect...
A new generation of lightweight subsea structures is planned for application in oil and gas producti...
The influence of geometrical factors on the galvanic current distribution for the magnesium alloy AZ...
An investigation was carried out into the galvanic corrosion of magnesium alloy AZ91D in contact wit...
The galvanic corrosion of the (Cu - Fe), (Cu - Zn) and (Fe - Zn) couples have been investigated in 3...
The anisotropic deposit film formed during the galvanic corrosion can impede the mass transfer of th...
The local electrochemical properties of galvanic corrosion for three coupled metals in a desalinatio...
The galvanic corrosion behavior of three metal alloys commonly used in water desalination plants was...
Here, we present for the first time, an experimentally validated numerical model for a galvanic coup...
Galvanic corrosion behavior of A 516 steel coupled to alloy C-22 and Ti Gr-12, respectively was eval...
Many magnesium alloys exhibit microgalvanic corrosion due to anodic and cathodic reactions that occu...
The subsea industry is moving its operations down onto the seabed. With this new direction in produc...
Here a time dependent numerical model aimed to investigate the role of mechanical deformation on the...
Mathematical nalysis for the mean current density has been completed for one gen-eral and two limiti...
Galvanic corrosion on samples of AZ91D magnesium alloy coupled with 2A12 aluminum alloy during neutr...
The objective of this research was to develop a method for a-priori quantitative prediction of elect...
A new generation of lightweight subsea structures is planned for application in oil and gas producti...
The influence of geometrical factors on the galvanic current distribution for the magnesium alloy AZ...
An investigation was carried out into the galvanic corrosion of magnesium alloy AZ91D in contact wit...
The galvanic corrosion of the (Cu - Fe), (Cu - Zn) and (Fe - Zn) couples have been investigated in 3...
The anisotropic deposit film formed during the galvanic corrosion can impede the mass transfer of th...
The local electrochemical properties of galvanic corrosion for three coupled metals in a desalinatio...
The galvanic corrosion behavior of three metal alloys commonly used in water desalination plants was...
Here, we present for the first time, an experimentally validated numerical model for a galvanic coup...
Galvanic corrosion behavior of A 516 steel coupled to alloy C-22 and Ti Gr-12, respectively was eval...
Many magnesium alloys exhibit microgalvanic corrosion due to anodic and cathodic reactions that occu...
The subsea industry is moving its operations down onto the seabed. With this new direction in produc...
Here a time dependent numerical model aimed to investigate the role of mechanical deformation on the...
Mathematical nalysis for the mean current density has been completed for one gen-eral and two limiti...
Galvanic corrosion on samples of AZ91D magnesium alloy coupled with 2A12 aluminum alloy during neutr...
The objective of this research was to develop a method for a-priori quantitative prediction of elect...
A new generation of lightweight subsea structures is planned for application in oil and gas producti...