The interface adhesion strength (or interface toughness) of a thin film/substrate system is often assessed by the micro-scratch test. For a brittle film material, the interface adhesion strength is easily obtained through measuring the scratch driving forces. However, to measure the interface adhesion strength (or interface toughness) for a metal thin film material (the ductile material) by the microscratch test is very difficult, because intense plastic deformation is involved and the problem is a three-dimensional elastic-plastic one. In the present research, using a double-cohesive zone model, the failure characteristics of the thin film/substrate system can be described and further simulated. For a steady-state scratching process, a thr...
The periodic cracking technique for determining the work of adhesion of thin metallic films was appl...
Adhesive failure and the attendant delamination of a thin film on a substrate is controlled by the f...
Thin brittle coatings with thickness of a few nanometres deposited on flexible polymer substrates fo...
There are two main issues regarding thin film debonding. The first is the nucleation of interfacial ...
In order to describe the interfacial fracture behaviors of the metal thin film with nano- or microsc...
Peeling experiments for aluminum thin film along the Al2O3 substrate are carried out, and the variat...
The assessment of adhesion property of thin films by scratch test method is still a big challenge, r...
In order to describe the interfacial fracture behaviors of the metal thin film with nano- or microsc...
Two types of peeling experiments are performed in the present research. One is for the Al film/Al2O3...
Scratching of thin coatings on hard substrates is studied experimentally and numerically, in the lat...
Surfaces are more and more used to add specific properties to materials towards multifunctional sys...
In this work, a series of two-dimensional plane-strain finite element analyses was conducted to furt...
In this work, a series of two-dimensional plane-strain finite element analyses was conducted to furt...
Abstract. A cohesive zone model is proposed and analyzed for steady-state peeling of a thin rate-ind...
Thin films and multilayered structures are increasingly used in the industry. One of the important m...
The periodic cracking technique for determining the work of adhesion of thin metallic films was appl...
Adhesive failure and the attendant delamination of a thin film on a substrate is controlled by the f...
Thin brittle coatings with thickness of a few nanometres deposited on flexible polymer substrates fo...
There are two main issues regarding thin film debonding. The first is the nucleation of interfacial ...
In order to describe the interfacial fracture behaviors of the metal thin film with nano- or microsc...
Peeling experiments for aluminum thin film along the Al2O3 substrate are carried out, and the variat...
The assessment of adhesion property of thin films by scratch test method is still a big challenge, r...
In order to describe the interfacial fracture behaviors of the metal thin film with nano- or microsc...
Two types of peeling experiments are performed in the present research. One is for the Al film/Al2O3...
Scratching of thin coatings on hard substrates is studied experimentally and numerically, in the lat...
Surfaces are more and more used to add specific properties to materials towards multifunctional sys...
In this work, a series of two-dimensional plane-strain finite element analyses was conducted to furt...
In this work, a series of two-dimensional plane-strain finite element analyses was conducted to furt...
Abstract. A cohesive zone model is proposed and analyzed for steady-state peeling of a thin rate-ind...
Thin films and multilayered structures are increasingly used in the industry. One of the important m...
The periodic cracking technique for determining the work of adhesion of thin metallic films was appl...
Adhesive failure and the attendant delamination of a thin film on a substrate is controlled by the f...
Thin brittle coatings with thickness of a few nanometres deposited on flexible polymer substrates fo...