In recent studies, nanoindentation experiments combined with the Oliver and Pharr method (OP method) are frequently used to measure the mechanical properties of “one-dimensional” structural materials (micro/nanowires and nanobelts) regardless of the corresponding assumptions of the OP method. This article reports the numerical simulation studies of the nanoindentations of wire structural materials on elastic-plastic substrates using dimensional analysis and the finite element method. We find that the measured hardness and Young’s modulus of wire structural materials are significantly influenced by their geometries and indenters as well as the mechanical properties of substrates and wires.Department of Mechanical EngineeringAuthor name used ...
When fabricating nanowires in a doubly-clamped beam configuration it is possible for a residual axia...
Purpose: Metallic glass wire products are known for their high fatigue strength and their interestin...
Nanoindentation techniques have been widely used to measure thin film mechanical properties. One of ...
Author name used in this publication: S. Q. ShuAuthor name used in this publication: J. Lu2008-2009 ...
Nanomechanical properties of indium nanowires like structures fabricated on quartz substrate by tren...
Nanomechanical properties of indium nanowires like structures fabricated on quartz substrate by tren...
The hardness and elastic modulus of a silver nanowire was measured using a nanoindenter. It was foun...
The hardness and elastic modulus of a silver nanowire was measured using a nanoindenter. It was foun...
The elastic properties of metallic and semiconducting nanowires were analyzed by different technique...
Instrumented nanoindentation tests have reached an effective level of theoretical and practical know...
Click on the DOI link below to access the article (may not be free).In this article, the sizes of th...
Nanobending tests are widely used in the mechanical characterization of nanomaterials. However, nano...
The principal strengths of the nanoindentation technique, which is used extensively to measure the m...
Nanomechanical properties of indium nanowires like structures fabricated on quartz substrate by tren...
Nanoindentation is a widely recognized method for characterizing the mechanical properties of thin f...
When fabricating nanowires in a doubly-clamped beam configuration it is possible for a residual axia...
Purpose: Metallic glass wire products are known for their high fatigue strength and their interestin...
Nanoindentation techniques have been widely used to measure thin film mechanical properties. One of ...
Author name used in this publication: S. Q. ShuAuthor name used in this publication: J. Lu2008-2009 ...
Nanomechanical properties of indium nanowires like structures fabricated on quartz substrate by tren...
Nanomechanical properties of indium nanowires like structures fabricated on quartz substrate by tren...
The hardness and elastic modulus of a silver nanowire was measured using a nanoindenter. It was foun...
The hardness and elastic modulus of a silver nanowire was measured using a nanoindenter. It was foun...
The elastic properties of metallic and semiconducting nanowires were analyzed by different technique...
Instrumented nanoindentation tests have reached an effective level of theoretical and practical know...
Click on the DOI link below to access the article (may not be free).In this article, the sizes of th...
Nanobending tests are widely used in the mechanical characterization of nanomaterials. However, nano...
The principal strengths of the nanoindentation technique, which is used extensively to measure the m...
Nanomechanical properties of indium nanowires like structures fabricated on quartz substrate by tren...
Nanoindentation is a widely recognized method for characterizing the mechanical properties of thin f...
When fabricating nanowires in a doubly-clamped beam configuration it is possible for a residual axia...
Purpose: Metallic glass wire products are known for their high fatigue strength and their interestin...
Nanoindentation techniques have been widely used to measure thin film mechanical properties. One of ...