Stress corrosion cracking (SCC) is a well known form of environmental attack in low carat gold jewellery. It is desirable to have a quick, easy and cost effective way to detect SCC in alloys and prevent them from being used and later failing in their application. A facile chemical method to investigate SCC of 9 carat gold alloys is demonstrated. It involves a simple application of tensile stress to a wire sample in a corrosive environment such as 1–10 % FeCl3 which induces failure in less than 5 minutes. In this study three quaternary (Au, Ag, Cu and Zn) 9 carat gold alloy compositions were investigated for their resistance to SCC and the relationship between time to failure and processing conditions is studied. It is envisaged that the use...
Alloy 260 brass specimens under stress were exposed at room temperature to 15 N aqueous ammonia solu...
The stress corrosion cracking (SCC) behaviour of solution heat-treated as-cast Mg0.1Zr, Mg1Mn, Mg0.1...
A case study of Stress Corrosion Cracking or SCC is a part of this project title. Stress corrosion c...
Stress corrosion cracking (SCC) is a well known form of environmental attack in low carat gold jewel...
Gold alloys used in jewellery applications are designed to improve mechanical properties and reduce ...
Gold alloys used in jewellery applications are designed to improve mechanical properties and reduce ...
Stress Corrosion Cracking (SCC) is a materials degradation mechanism known to affect stainless steel...
Stress and high temperature influence titanium alloys specially while they are in contact with other...
Lower carat gold alloys, specifically 9 carat gold alloys, containing less than 40 % gold, and alloy...
Lower carat gold alloys, specifically 9 carat gold alloys, containing less than 40 % gold, and alloy...
The development of standardised methods of testing is a key element in the prevention of stress corr...
Stress corrosion cracking (SCC) is a phenomenon in which the cracking of a metal alloy usually resul...
International audienceExperimental techniques used to investigate stress corrosion cracking (SCC) ar...
This research program has had two major areas of focus that are related: (1) alloy corrosion and (2)...
Three commercial gold-based dental alloys and three constant-nobility ternary alloys (Au-Ag-Cu) were...
Alloy 260 brass specimens under stress were exposed at room temperature to 15 N aqueous ammonia solu...
The stress corrosion cracking (SCC) behaviour of solution heat-treated as-cast Mg0.1Zr, Mg1Mn, Mg0.1...
A case study of Stress Corrosion Cracking or SCC is a part of this project title. Stress corrosion c...
Stress corrosion cracking (SCC) is a well known form of environmental attack in low carat gold jewel...
Gold alloys used in jewellery applications are designed to improve mechanical properties and reduce ...
Gold alloys used in jewellery applications are designed to improve mechanical properties and reduce ...
Stress Corrosion Cracking (SCC) is a materials degradation mechanism known to affect stainless steel...
Stress and high temperature influence titanium alloys specially while they are in contact with other...
Lower carat gold alloys, specifically 9 carat gold alloys, containing less than 40 % gold, and alloy...
Lower carat gold alloys, specifically 9 carat gold alloys, containing less than 40 % gold, and alloy...
The development of standardised methods of testing is a key element in the prevention of stress corr...
Stress corrosion cracking (SCC) is a phenomenon in which the cracking of a metal alloy usually resul...
International audienceExperimental techniques used to investigate stress corrosion cracking (SCC) ar...
This research program has had two major areas of focus that are related: (1) alloy corrosion and (2)...
Three commercial gold-based dental alloys and three constant-nobility ternary alloys (Au-Ag-Cu) were...
Alloy 260 brass specimens under stress were exposed at room temperature to 15 N aqueous ammonia solu...
The stress corrosion cracking (SCC) behaviour of solution heat-treated as-cast Mg0.1Zr, Mg1Mn, Mg0.1...
A case study of Stress Corrosion Cracking or SCC is a part of this project title. Stress corrosion c...